Specifications
Brand Name :
ZEIT
Model Number :
ALD-SEM-X—X
Certification :
Case by case
Place of Origin :
Chengdu, P.R.CHINA
MOQ :
1set
Price :
Case by case
Payment Terms :
T/T
Supply Ability :
Case by case
Delivery Time :
Case by case
Packaging Details :
Wooden case
Weight :
Customizable
Size :
Customizable
Guarantee period :
1 year or case by case
Customizable :
Available
Shipping Terms :
By Sea / Air / Multimodal Transport
Description

Atomic Layer Deposition in Semiconductor Industry


Applications

Applications Specific Purpose
Semiconductor

Logic device (MOSFET), High-K gate dielectrics / gate electrode

High-K capacitive material / capacitive electrode of Dynamic Random Access
Memory (DRAM)

Metal interconnection layer, metal passivation layer, metal seed crystal layer, metal
diffusion barrier layer

Non-volatile memory:flash memory, phase change memory, resistive random access
memory, ferroelectric memory, 3D packaging, OLED passivation layer,etc.


Working Principle
Atomic layer deposition (ALD) technology, also known as atomic layer epitaxy (ALE) technology, is a chemical

vapor film deposition technology based on ordered and surface self-saturated reaction. ALD is applied in

semiconductor field. As Moore’s Law evolves constantly and the feature sizes and etching grooves of integrated

circuits have been constantly miniaturizing, the smaller and smaller etching grooves have been bringing severe

challenges to the coating technology of grooves and their side walls.Traditional PVD and CVD process have been

unable to meet the requirements of superior step coverage under narrow line-width. ALD technology is playing an

increasingly important role in semiconductor industry due to its excellent shape-keeping, uniformity and higher step

coverage.

Features

Model ALD-SEM-X—X
Coating film system AL2O3, TiO2, ZnO, etc
Coating temperature range Normal temperature to 500℃ (Customizable)
Coating vacuum chamber size

Inner diameter: 1200mm, Height: 500mm (Customizable)

Vacuum chamber structure According to customer’s requirements
Background vacuum <5×10-7mbar
Coating thickness ≥0.15nm
Thickness control precision ±0.1nm
Coating size 200×200mm² / 400×400mm² / 1200×1200 mm², etc
Film thickness uniformity ≤±0.5%
Precursor and carrier gas

Trimethylaluminum, titanium tetrachloride, diethyl zinc, pure water,
nitrogen, etc.

Note: Customized production available.


Coating Samples

MOSFET Semiconductor Detector Systems Atomic Layer Deposition Equipment ISOMOSFET Semiconductor Detector Systems Atomic Layer Deposition Equipment ISO

Process Steps
→ Place the substrate for coating into the vacuum chamber;
→ Vacuumize the vacuum chamber at high and low temperature, and rotate the substrate synchronously;
→ Start coating: the substrate is contacted with precursor in sequence and without simultaneous reaction.
→ Purge it with high-purity nitrogen gas after each reaction;
→ Stop rotating the substrate after the film thickness is up to standard and the operation of purging and cooling is

completed, then take out the substrate after the vacuum breaking conditions are met.

Our Advantages
We are manufacturer.
Mature process.
Reply within 24 working hours.

Our ISO Certification
MOSFET Semiconductor Detector Systems Atomic Layer Deposition Equipment ISO

Parts Of Our Patents
MOSFET Semiconductor Detector Systems Atomic Layer Deposition Equipment ISOMOSFET Semiconductor Detector Systems Atomic Layer Deposition Equipment ISO

Parts Of Our Awards and Qualifications of R&D

MOSFET Semiconductor Detector Systems Atomic Layer Deposition Equipment ISO MOSFET Semiconductor Detector Systems Atomic Layer Deposition Equipment ISO









Send your message to this supplier
Send Now

MOSFET Semiconductor Detector Systems Atomic Layer Deposition Equipment ISO

Ask Latest Price
Watch Video
Brand Name :
ZEIT
Model Number :
ALD-SEM-X—X
Certification :
Case by case
Place of Origin :
Chengdu, P.R.CHINA
MOQ :
1set
Price :
Case by case
Contact Supplier
video
MOSFET Semiconductor Detector Systems Atomic Layer Deposition Equipment ISO

ZEIT Group

Active Member
5 Years
sichuan, chengdu
Since 2018
Business Type :
Manufacturer, Exporter, Seller
Total Annual :
$10,000,000-$15,000,000
Employee Number :
120~200
Certification Level :
Active Member
Contact Supplier
Submit Requirement