Material :
UNS S32750,S31803, S32205, S32760
Standard :
SA789,A790
Type :
Seamless,Welded
OD :
1/4inch~24inch
Wall Thickness :
SCH10S , SCH10, SCH20, SCH30, SCH40S...
Application :
Heat exchangers and coolers
Surface Treatment :
Varnish, Oil-dip, Passivation, Phosphating, Shot Blasting
Delivery Status :
Annealed, normalized, normalized+Tempered, etc
Description

SA789 UNS S32750 Stainless Steel Tubing Super Duplex Stainless Steel Pipe / Tube 25.4 * 2.11mm

Product Standard: ASME SA789
Main steel grades:
UNS S32750,S31803, S32205, S32760

Application: For heat exchangers and coolers and devices that are resistant to seawater, such as high temperature and concentrated nitric acid, such as oil refining, fertilizer, papermaking, petroleum, and Foundry

Features:

1.Superior resistance to general and local corrosion, especially to stress corrosion, pitting corrosion, crevice corrosion, corrosion fatigue and abrasion & corrosion.

2.Good weldability

3.Good mechanical properties

4.Excellent intergranular corrosion resistance

5.High cost-effectiveness, long life time

Chemical Composition & Physical Properties:

Grade

C

max

Si

max

Mn

max

P

max

S

max

Cr Ni Mo N
UNS S32750 0.030 0.8 1.2 0.030 0.015 24.0-26.0 6.0-8.0 3.0-5.0 0.24-0.32
UNS S31803 0.030 1.0 2.0 0.020 0.020 21.0-23.0 4.5-6.5 2.5-3.5 0.08-0.20
UNS S31500 0.030 1.0 1.2-2.0 0.030 0.030 18.0-19.0 4.5-5.5 2.5-3.5 0.05-0.10

Grade Y.S.MPa min T.S.Mpa min Elongation % Hardness HRC
UNS S32750 550 800 15 20
UNS S31803 450 620 25 20
UNS S31500 440 630 30 20

Mark: As required.

Inspection and Test: chemical composition test, mechanical properties test(tensile, yield, elongation), process properties test(flatting, flaring, bending, hardness, impact, etc.), appearance and size test, non-destructive inspection test, hydrostastic test.

Delivery status: Annealed, normalized, normalized+Tempered, etc.

Surface treatment: oil impregnation, paint, passivation, phosphating, shot blasting etc.

Packing: Exporting package/wooden box /as requirement.

Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube

Send your message to this supplier
Send Now

Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube

Ask Latest Price
Brand Name :
Y & G
MOQ :
Negotiation
Payment Terms :
L/C, T/T
Supply Ability :
8000MT/Month
Delivery Time :
25-35 days
Packaging Details :
Exporting package/wooden box / per customers’ requirement
Contact Supplier
Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube
Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube
Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube
Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube
Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube

Y & G International Trading Company Limited

Active Member
9 Years
beijing, beijing
Since 2003
Business Type :
Manufacturer, Trading Company
Total Annual :
10000000-20000000
Employee Number :
20~30
Certification Level :
Active Member
Contact Supplier
Submit Requirement