Steel 1.4404 Type 01 EN1092-1 Steel Plate Flange X2CrNiMo17-12-2
Product Overview
Steel 1.4404 Type 01 EN1092-1 Plate flange made from austenitic stainless steel grade X2CrNiMo17-12-2.
Material Specifications
| Grade: |
X2CrNiMo17-12-2 |
| Number: |
1.4404 |
| Classification: |
Austenitic stainless steel |
| Density: |
8 g/cm³ |
Applicable Standards
- EN 10088-2:2005 Stainless steels - Technical delivery conditions for sheet/plate and strip
- EN 10088-3:2005 Stainless steels - Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products
- EN 10028-7:2007 Flat products made of steels for pressure purposes - Stainless steels
- EN 10216-5:2014 Seamless steel tubes for pressure purposes - Stainless steel tubes
- EN 10217-7:2005 Welded steel tubes for pressure purposes - Stainless steel tubes
- EN 10296-2:2005 Welded circular steel tubes for mechanical and general engineering purposes - Stainless steel
- EN 10253-3:2008 Butt-welding pipe fittings - Wrought austenitic and austenitic-ferritic stainless steels
- EN 10253-4:2008 Butt-welding pipe fittings - Wrought austenitic and austenitic-ferritic stainless steels with inspection
- EN 10272:2007 Stainless steel bars for pressure purposes
- EN 10269:1999 Steels and nickel alloys for fasteners
- EN 10263-5:2001 Steel rod, bars and wire for cold heading and cold extrusion
- EN 10250-4:2000 Open steel die forgings for general engineering purposes
- EN 10297-2:2005 Seamless circular steel tubes for mechanical and general engineering purposes
- EN 10222-5:2000 Steel forgings for pressure purposes
- EN 10088-1:2005 Stainless steels - List of stainless steels
- EN 10088-4:2009 Stainless steels for construction purposes
- EN 10088-5:2009 Stainless steels for construction purposes
Chemical Composition (%) - EN 10088-2:2005
Note: Particular ranges of sulphur content may provide improvement of specific properties. For machinability: 0.015% to 0.030%; for weldability: 0.008% to 0.030%; for polishability: max 0.015%.
| Element |
Content |
| C |
max 0.03 |
| Si |
max 1 |
| Mn |
max 2 |
| Ni |
10 - 13 |
| P |
max 0.045 |
| S |
max 0.015 |
| Cr |
16.5 - 18.5 |
| Mo |
2 - 2.5 |
| N |
max 0.11 |
Mechanical Properties
| Tensile Strength (MPa) +A |
490-700 |
| Tensile Strength (MPa) +AT |
490-690 |
| Tensile Strength (MPa) +AT+C |
750-780 |
| 0.2% Proof Strength (MPa) +AT |
190 |
| 0.2% Proof Strength (MPa) +A |
190-235 |
| Impact Energy (J) Transverse +A at +20°C |
60 |
| Impact Energy (J) Transverse +A at -196°C |
60 |
| Impact Energy (J) Longitudinal +A at +20°C |
100 |
| Elongation at Fracture (%) +A |
30-45 |
| Elongation at Fracture (%) Longitudinal +AT |
40 |
| Nominal Diameter (mm) |
2 - 50 |
| Reduction in Cross Section (%) |
63-68 |
| Brinell Hardness (HB) +A |
215 |
| Brinell Hardness (HB) +AT |
200 |
Material Properties
Resistance to intergranular corrosion: in delivery condition - yes; in sensitized condition - yes.
Steel shall not be applied at metal temperatures lower than -196°C.
Equivalent Grades
| Region |
Designation |
| EU EN |
X2CrNiMo17-12-2 |
| USA |
316L |
| Germany DIN |
X2CrNiMo17-13-2 |
| Japan JIS |
SUS316, SUS316L |
| France AFNOR |
Z2CND17-12, Z3CND17-11-02, Z3CND18-12-02 |
| England BS |
316S11 |
| Italy UNI |
X2CrNiMo17-12, X2CrNiMo17-17-12 |
| China GB |
00Cr17Ni14Mo2, 0Cr18Ni12Mo2Ti |
| Sweden SS |
2348 |
| Poland PN |
00H17N13M2, 00H17N14M2 |
| Czechia CSN |
17349 |
| Finland SFS |
750 |
| Austria ONORM |
X2CrNiMo17-13-2KKW |
| International ISO |
Type19 |