Shock-proof & Wear Resistant Axle-centre Alloy 40ХНЮ-ВИ, ЭП793 Russia, 3J40 China Grade
Size range:
cold drawn wire: 0.2-6.0mm
Hot rolled/forged bar: 6-100mm
Shock-proof & Wear Resistant axle-centre alloy(YB/T5243-1993) Relative Grade:40ХНЮ-ВИ,ЭП793 Russia |
Grade and Chemical Composition (see Table1) Table1 Grade and Chemical Composition Grade | Chemical Composition (%) | C | P | S | Mn | Si | Fe | Cr | A1 | Ce① | Ni | ≤ | 3J40 | 0.03 | 0.010 | 0.010 | 0.10 | 0.20 | 0.50 | 39.0~41.0 | 3.30~3.50 | 0.10~0.2 | Balance | ①Based on addition Mechanical Property (see Table 2) Table 2 Mechanical Property Statue | Vickers Hardness/ HV | Commended Heat Treatment | Bend Test The radius of the mandrel is twice as the diameter of the alloy | I | Ⅱ | Ⅲ | | Cold Drawing | 450~510 | | Bend 90 degrees. No cracks and broken on the outside of the bending | Cold Drawn & Aging | 780~830 | >830~880 | >880 | 480~540°C Keep warm for 5h | | Note: 1.The default hardness classification of the alloy wire in cold drawing & aging status is class II. Physical Property (see Table 3—Table 5) Table 3 Coefficient of Linear Expansion State | Coefficient of Linear Expansion/(10-6/K) | 20~55℃ | 20~100℃ | 20~200℃ | 20~300℃ | 20~400℃ | 20~500℃ | Solid Solution | 12.2~12.7 | 12.4~12.5 | 12.6~12.8 | 13.0~13.1 | 13.5~13.6 | 13.8~14.0 | Solid Solution&aging | 11.0~11.5 | 11.9~12.0 | 12.0~12.2 | 12.4~12.5 | 12.7~12.8 | 13.1~13.3 | Cold Drawn & aging | 11.6 | 12.0 | 12.1 | 12.4 | 12.8 | 13.3 | Table 4 Modulus of Elasticity & Frequency Temperature Coefficient State | Modulus of Elasticity | Temperature Coefficient βf/(10-6℃) | Mechanical Quality Factor Q20℃ | 20~-40℃ | 20~100℃ | Solid Solution +80% Strain Rate | 176500~196000 | | | | Solid Solution +80% Strain Rate+Aging 5h | 225500~235500 | -103~-106 | -104~-110 | 49000~51000 | Table 5 Magnetic Susceptibility & Resistivity State | Magnetic Susceptibility | Resistivity/(μΩ•m) | Density/(g/cm3) | H=40KA/m | H:80KA/m | Solid Solution | 3.5~4.5 | 3.5~4.6 | | 7.6 | Solid Solution+ Aging | 3.8~4.0 | 2.4~4.2 | | | Solid Solution+ Cold Drawing | 2.8~3.0 | | 1.21 | | Solid Solution +69% Strain Rate+Aging | | | 0.78 | | Corrosion Resisting Property (See Table 5) Table 5 Corrosion Resisting Property State | Salt Fog Test | Long-time Store in The Air | Cold Drawing+ Solid Solution+Aging | No corrosion after 240 hours (Tested by the buyer per JB1606) | No corrosion | |
 Usage: It is applied to produce the axle-centre of instrument and meter as well as the axle-centre of the staff |