Specifications
Brand Name :
Zhonggong Special Metallurgy
Model Number :
GH3039 alloy
Place of Origin :
China
Price :
Price is negotiated based on the required specifications and quantity
Payment Terms :
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability :
5000 tons per month
Delivery Time :
5-8 working days, depending on the parameters required for negotiation
Packaging Details :
Standard export packaging, or packaging as required
MOQ :
100KG
Certification :
ISO Certificate
Composition :
Nickel-based superalloy containing Chromium, Cobalt, Iron, and other elements
Density :
8.23 g/cm³
Melting Point :
1320-1370°C (2408-2498°F)
Tensile Strength :
850-1100 MPa (at room temperature)
Yield Strength (0.2% offset) :
450-700 MPa
Elongation :
30-50%
Thermal Conductivity :
9.8 W/m·K (at 100°C)
Specific Heat Capacity :
Specific Heat Capacity
Coefficient of Thermal Expansion :
13.6 µm/m·K (20-100°C)
Electrical Resistivity :
1.10 µΩ·m (at 20°C)
Magnetic Properties :
Non-magnetic
Description

GH3039 alloy, a high-performance nickel-based superalloy, excels in demanding environments due to its exceptional mechanical strength, oxidation resistance, and corrosion resistance. Composed primarily of nickel, chromium, cobalt, and iron, GH3039 maintains its integrity and reliability at temperatures up to approximately 1370°C (2498°F). It offers excellent creep and fatigue resistance, crucial for applications in gas turbines, aerospace components, and chemical processing equipment where prolonged exposure to high temperatures and aggressive environments is common. GH3039 alloy's non-magnetic properties and ability to maintain strength over extended service life make it a preferred choice for critical industrial applications requiring high performance and reliability under extreme conditions.

Here's a detailed composition table for GH3039 alloy:

Element Composition (%)
Nickel (Ni) 51.0 - 55.0
Chromium (Cr) 19.0 - 22.0
Cobalt (Co) 15.0 - 20.0
Iron (Fe) 5.0 - 9.0
Molybdenum (Mo) 2.5 - 3.5
Titanium (Ti) ≤ 0.70
Aluminum (Al) ≤ 0.60
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 0.50
Silicon (Si) ≤ 0.50
Phosphorus (P) ≤ 0.015
Sulfur (S) ≤ 0.010
Boron (B) ≤ 0.006

GH3039 alloy is primarily composed of nickel, chromium, cobalt, and iron, with minor additions of molybdenum, titanium, aluminum, and trace elements to achieve its desired properties for high-temperature and corrosion-resistant applications.

Gh3039 Corrosion Resistant Nickel Based Superalloy 8.23 g/cm3 high performance

Gh3039 Corrosion Resistant Nickel Based Superalloy 8.23 g/cm3 high performance

Send your message to this supplier
Send Now

Gh3039 Corrosion Resistant Nickel Based Superalloy 8.23 g/cm3 high performance

Ask Latest Price
Brand Name :
Zhonggong Special Metallurgy
Model Number :
GH3039 alloy
Place of Origin :
China
Price :
Price is negotiated based on the required specifications and quantity
Payment Terms :
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability :
5000 tons per month
Contact Supplier
Gh3039 Corrosion Resistant Nickel Based Superalloy 8.23 g/cm3 high performance
Gh3039 Corrosion Resistant Nickel Based Superalloy 8.23 g/cm3 high performance

Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.

Active Member
2 Years
jiangsu, wuxi
Since 2010
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Other, Seller, Trading Company
Total Annual :
1000000-1500000
Employee Number :
100~200
Certification Level :
Active Member
Contact Supplier
Submit Requirement