Specifications
Brand Name :
Zhonggong Special Metallurgy
Model Number :
GH5188 Alloy
Place of Origin :
China
MOQ :
100KG
Price :
Price is negotiated based on the required specifications and quantity
Payment Terms :
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability :
5000 tons per month
Delivery Time :
5-8 working days, depending on the parameters required for negotiation
Packaging Details :
Standard export packaging, or packaging as required
Certification :
ISO Certificate
Material Type :
Nickel-based Superalloy
Chemical Composition :
Ni, Cr, Co, Mo, W, Ti, Al, other elements
Density :
~8.4 g/cm³
Tensile Strength :
~1000 MPa
Yield Strength :
~850 MPa
Temperature Range :
Up to 980°C (1800°F)
Oxidation Resistance :
Excellent
Corrosion Resistance :
High
Applications :
Aerospace, power generation, chemical processing
Description

GH5188 Alloy is a high-performance nickel-based superalloy specifically engineered for demanding applications where extreme conditions are prevalent. This alloy is characterized by its superior high-temperature strength, excellent resistance to oxidation and corrosion, and robust mechanical properties.

Key Features:

  • Composition: The alloy comprises nickel (Ni) as the base element, along with chromium (Cr), cobalt (Co), molybdenum (Mo), tungsten (W), titanium (Ti), and aluminum (Al). These elements contribute to its exceptional hardness and stability.
  • Temperature Resistance: GH5188 maintains its mechanical integrity and performance up to 980°C (1800°F), making it suitable for high-temperature environments.
  • Mechanical Properties: It offers outstanding tensile and yield strength, ensuring reliability and durability under extreme conditions. The alloy's ability to withstand stress and thermal cycling makes it ideal for critical applications.
  • Corrosion and Oxidation Resistance: The alloy's composition provides excellent resistance to oxidation and corrosion, even in harsh environments, prolonging the lifespan of components.
  • Applications: Commonly used in aerospace components, turbine blades, exhaust systems, and other high-stress parts requiring superior performance and longevity.
  • Heat Treatment: GH5188 can be heat-treated to achieve optimal mechanical properties, offering flexibility in processing and manufacturing.

GH5188 Alloy's combination of high strength, thermal stability, and resistance to harsh environments ensures it meets the stringent requirements of advanced industrial and aerospace applications.

Here’s a typical composition table for GH5188 Alloy:

Element Composition (%)
Nickel (Ni) Balance
Chromium (Cr) 19.0 - 21.0
Cobalt (Co) 10.0 - 12.0
Molybdenum (Mo) 3.5 - 4.5
Tungsten (W) 3.0 - 4.0
Titanium (Ti) 2.0 - 2.5
Aluminum (Al) 1.5 - 2.0
Carbon (C) ≤ 0.08
Boron (B) ≤ 0.01
Silicon (Si) ≤ 0.50
Manganese (Mn) ≤ 0.50

These values are approximate and can vary based on the specific production standards and requirements.

GH5188 Alloy Nickel Based Superalloy High Strength Oxidation Resistance

Send your message to this supplier
Send Now

GH5188 Alloy Nickel Based Superalloy High Strength Oxidation Resistance

Ask Latest Price
Watch Video
Brand Name :
Zhonggong Special Metallurgy
Model Number :
GH5188 Alloy
Place of Origin :
China
MOQ :
100KG
Price :
Price is negotiated based on the required specifications and quantity
Payment Terms :
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Contact Supplier
video
GH5188 Alloy Nickel Based Superalloy High Strength Oxidation Resistance
GH5188 Alloy Nickel Based Superalloy High Strength Oxidation Resistance

Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.

Active Member
2 Years
jiangsu, wuxi
Since 2010
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Other, Seller, Trading Company
Total Annual :
1000000-1500000
Employee Number :
100~200
Certification Level :
Active Member
Contact Supplier
Submit Requirement