Specifications
Brand Name :
DINGSCO
Model Number :
According to customers requirements
Certification :
ISO 9001:2015,PED 2014/68/EU,API 6A,API-20B,TSG,NORSOK
Place of Origin :
China
MOQ :
Negotiable
Price :
Negotiable
Payment Terms :
T/T
Supply Ability :
Negotiable
Delivery Time :
(Sample Order) 7 days
Packaging Details :
According to Customers' Requests
Product Name :
Nickel Alloy Discs
Grade :
Inconel 718
UNS :
NO7718
Density :
8.2g/cm3
Melting Point :
1260℃-1336℃
Special Heat :
435J/kg・K
Description

‌Inconel 718 Forged Round Discs | Aerospace-Grade Superalloy | Precision Components


NickInconel 718 (UNS N07718 / W.Nr.2.4668) forged discs are high-performance nickel-chromium-niobium alloy components, engineered via precision controlled forging and optimized heat treatment for extreme high-stress, moderate-to-high temperature service. As a precipitation-hardened superalloy, its core strength comes from the formation of fine γ'' (Ni₃Nb) and secondary γ' (Ni₃Al/Ti) strengthening phases, delivering unrivaled tensile strength, fatigue resistance, creep/rupture performance and structural stability.

Core Material & Performance Advantages

1. Exceptional High-Strength (Precipitation-Hardened State)

  • Room temperature mechanicals: Tensile strength (Rm) 1100–1200 MPa, Yield strength (Rp0.2) ≥965 MPa, far exceeding conventional nickel alloys and stainless steels;
  • High-temperature retention: Retains 70%+ of room-temperature strength at 650°C long-term service, with excellent creep and rupture resistance (1000+ hours under rated stress/heat);
  • Permanent strength: Precipitation hardening forms stable intermetallic phases, no performance attenuation during long-term service, avoiding structural failure of critical components.

2. Superior Fatigue & Thermal Shock Resistance

  • All-around fatigue performance: Excellent high-cycle/low-cycle fatigue and thermal fatigue resistance, adapted to the cyclic mechanical/thermal loads of rotating equipment (turbines, compressors);
  • Thermal shock stability: Low thermal expansion coefficient and good thermal conductivity, reducing internal stress under rapid temperature changes, no cracking or deformation;
  • High impact toughness: Charpy V-notch impact value ≥60 J at room temperature, retains high ductility even at liquid nitrogen temperature (-196°C), no cold brittleness for cryogenic applications.


Properties YS(Ksi) TS(Ksi) EL(%) HRC
Room Temperature 180 150 12 36
1200℉(<0.025-in) 140 115 - -
1200℉(>0.025-in ) 145 120 5 -



Chemical Composition:


Element Ni Cr S C Mn Si Mo Cu Co Al Nb B P
Minimum(%) 50 17 - - - - 2.8 - - 0.2 4.75 - -
Max(%) 55 21 0.015 0.08 0.35 0.35 3.3 0.3 1.0 0.8 5.5 0.006 0.015



Our QC Activities and Test Methods:


Chemical Analysis ASTM E1473ensile Test ASTM E8
Hardness Test ASTM E 10,E 18 PMl Examination DINGSCO SOP
Ultrasonic NDT BS EN 10228 Liquid Penetrant NDT ASTM E 165
Dimensional and inspection DINGSCO SOP Roughness Test DINGSCO SOP
Impact Test ASTM E 23 Low Temperature lmpact Test ASTM E 23
Creep and Stress Rupture Test ASTM E 139 Hydrogen Induced Cracking Test NACE TM-0284 *
Inter Granular Corrosion Test ASTM A 262 * Sulfide Stress Corrosion Cracking Test NACE TM-0177 *
Pitting and Crevice Corrosion Test ASTM G 48 * Macro Etching Test ASTM E 340*
Grain Size Test ASTM E 112 *

* Done by state own third party laboratory



‌Inconel 718 Forged Round Discs | Aerospace-Grade Superalloy | Precision Components



Send your message to this supplier
Send Now

‌Inconel 718 Forged Round Discs | Aerospace-Grade Superalloy | Precision Components

Ask Latest Price
Watch Video
Brand Name :
DINGSCO
Model Number :
According to customers requirements
Certification :
ISO 9001:2015,PED 2014/68/EU,API 6A,API-20B,TSG,NORSOK
Place of Origin :
China
MOQ :
Negotiable
Price :
Negotiable
Contact Supplier
video
‌Inconel 718 Forged Round Discs | Aerospace-Grade Superalloy | Precision Components
‌Inconel 718 Forged Round Discs | Aerospace-Grade Superalloy | Precision Components

Hunan Dinghan New Material Technology Co., LTD

Verified Supplier
3 Years
hunan, changsha
Since 1998
Business Type :
Manufacturer, Exporter, Seller
Total Annual :
70 million-100 million
Employee Number :
50~60
Certification Level :
Verified Supplier
Contact Supplier
Submit Requirement