SAPHIR 17 Decorative Chromium Plating Process
Performance & Features
- Self-regulating formula, free of solid catalyst.
- Outstanding gloss, exceptional throwing power and covering power.
- Operable under wide chromic anhydride concentration range: 175–300 g/L.
Equipment Requirements
| Item |
Specification |
| Plating Tank |
Steel tank lined with chromic acid resistant coating |
| Heating / Cooling System |
Direct or indirect heating; automatic temperature controller mandatory |
| Ventilation System |
Required; ductwork made of plastic-lined steel or plastic |
| Racks |
Nickel-plated copper rod; max current density 2–3 A/mm² |
| Anode |
Lead alloy anodes supplied by our factory recommended; Anode:Cathode area ratio = 1–1.5 : 1 |