Technical Specification
| Item |
Details |
| Material |
KTL-202 All-Hard Alloy |
| Main Alloy Composition |
Cr 7.8%, V 0.8%, Mo 2%, Co 0.8% |
| Heat Treatment Process |
- Quenching: 1020–1050°C
- Tempering: 550–570°C (≥3 times)
- Tail annealed at high temperature
|
| Hardness |
HRC 60± 2 |
| Key Features |
- Good wear resistance
- Stable hardness and toughness
- Reliable performance under standard working conditions
- Cost-effective solution
|