26MM Machine injection molding screw tip injection mold part Screw Tip Assembly
Technical Specification
| Item |
Details |
| Material |
KTL-202B All-Hard Alloy |
| Main Alloy Composition |
Cr 8.2%, V 1.2%, Mo 2%, Co 1% |
| Heat Treatment Process |
- Quenching: 1020–1050°C
- Tempering: 550–570°C (≥3 times)
- Tail annealed at high temperature
|
| Hardness |
HRC 58–60 |
| Key Features |
- Good wear resistance
- Stable hardness and toughness
- Reliable performance under standard working conditions