Specifications
Brand Name :
JINXING
Model Number :
Inconel X750 Spring Wire
Certification :
ISO 9001
Place of Origin :
China
MOQ :
5kg
Price :
10~200USD/kg
Payment Terms :
L/C, D/A, D/P, T/T, Western Union
Supply Ability :
5tons/M
Delivery Time :
25~35days
Packaging Details :
Plywood Case
Material :
Inconel X750 UNS N07750
Surface :
Black or Polished
Other named :
NiCr15Fe7TiAl, NC15FeTNbA, NCF750,GH4145
Heat Treatment :
Solution Annealing
Density :
8.25g/cm3
Melt Range :
1395~1425℃
Description

Inconel X750 Spring Wire / UNS N07750 / DIN W. Nr. 2.4669 high tensile strength

Inconel X-750 alloy is mainly used in the manufacture of corrosion-resistant planar wave springs, circumferential coil springs, helical compression springs, spring rings and seals for aeronautical engines operating below 540 °C.

Inconel X750 wire / UNS N07750 / DIN W. Nr. 2.4669

Inconel X-750(USA),NiCr15Fe7TiAl(Germany),NC15FeTNbA(France),NCF750(Japan),GH4145

Inconel X-750 alloy is mainly nickel-based super alloy aging with γ"[Ni3(Al, Ti, Nb)] phase. It has good corrosion resistance and oxidation resistance below 980 °C, and is higher than 800 °C. The strength, below 540 ° C has good resistance to slack, but also has good formability and weldability. The alloy is mainly used in the manufacture of aircraft engines that work below 800 ° C and require high strength and relaxation-resistant planar springs. Coil springs. Can also be used to make parts such as turbine blades

We can supply all kinds of Inconel X-750 bar, forging, ring, hot rolling plate, cold rolling plate, strip, tube and wire.

Plate and strip are generally supplied after hot rolling or cold rolling, annealing or solution, pickling and polishing.

Bars, forgings and rings may be supplied in the as forged or hot rolled condition, or in the solution treatment after forging; bars may be polished or turned smooth after solution, and may be placed in the cold drawn condition when required by the order.

The Inconel X-750 wire can be supplied in solution state; for the wire with nominal diameter or thickness less than 6.35mm, it can be supplied after solution and with cold drawing deformation of 50% - 65%; for the wire with nominal diameter or side length greater than 6.35mm, it can be supplied with cold drawing deformation of not less than 30% after solution treatment. For the wire with nominal diameter or side length no more than 0.65mm, it shall be supplied with cold drawing deformation no less than 15% after solution treatment as required.

Inconel x750 alloy

1. The forging temperature of alloy is from 1220 ℃ to 950 ℃. The alloy is treated by solution treatment after severe forming process.

2. The average grain size of the alloy is closely related to the deformation degree and final forging temperature.

3. The alloy has good welding performance and can be used for various welding. After welding, aging treatment can obtain the strength of near complete heat treatment.

4. The heat treatment of parts is carried out in neutral or reducing atmosphere without sulfur, so as to avoid vulcanization.

  • Bar
  • Wire
  • Sheet
  • Plate
  • Forgings
  • Pipe fittings
  • Flanges
  • Seamless & Welded pipe
  • Seamless Tube & Welded tube
  • Welding wire

Form ASTM
Rod, bar and forging ASTM B637

Inconel X750 wire Chemical composition :

% Ni Cr Fe C Mn Si S Ti Nb+Ta Al Co Cu
min 70 14 5         2.25 0.7 0.4    
max   17 9 0.08 1 0.5 0.01 2.75 1.2 1 1 0.5

Density 8.28 g/cm3
Melting range 1393-1427℃

Inconel X750 wire Application:

  • Nuclear reactors
  • Gas turbines
  • Rocket engines
  • Pressure vessels
  • Aircraft structures

Uns N07750 Nickel Based Superalloys , Inconel X750 Spring Wire For Nuclear Reactors

Send your message to this supplier
Send Now

Uns N07750 Nickel Based Superalloys , Inconel X750 Spring Wire For Nuclear Reactors

Ask Latest Price
Brand Name :
JINXING
Model Number :
Inconel X750 Spring Wire
Certification :
ISO 9001
Place of Origin :
China
MOQ :
5kg
Price :
10~200USD/kg
Contact Supplier
Uns N07750 Nickel Based Superalloys , Inconel X750 Spring Wire For Nuclear Reactors
Uns N07750 Nickel Based Superalloys , Inconel X750 Spring Wire For Nuclear Reactors
Uns N07750 Nickel Based Superalloys , Inconel X750 Spring Wire For Nuclear Reactors

JINXING MATECH CO LTD

Site Member
7 Years
Since 2007
Business Type :
Manufacturer, Distributor/Wholesaler, Importer, Exporter, Seller, Other
Total Annual :
5,000,000-10,000,000
Employee Number :
10~25
Certification Level :
Site Member
Contact Supplier
Submit Requirement