Specifications
Brand Name :
Zhonggong Special Metallurgy
Model Number :
GH600 Alloy
Place of Origin :
China
MOQ :
100KG
Price :
Price is negotiated based on the required specifications and quantity
Payment Terms :
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability :
5000 tons per month
Delivery Time :
5-8 working days, depending on the parameters required for negotiation
Packaging Details :
Standard export packaging, or packaging as required
Certification :
ISO Certificate
Material Type :
Nickel-based Superalloy
Density :
~8.4 g/cm³
Tensile Strength :
~750 MPa
Yield Strength :
~600 MPa
Temperature Range :
Up to 1100°C (2012°F)
Oxidation Resistance :
Excellent
Corrosion Resistance :
Good
Applications :
Aerospace, industrial gas turbines, exhaust systems
Heat Treatment :
Solution treated and aged
Form :
Bars, sheets, forgings, and custom shapes
Description

GH600 Alloy is a high-performance nickel-based superalloy specifically designed for applications requiring exceptional strength and durability at high temperatures. It provides outstanding mechanical properties, thermal stability, and oxidation resistance, making it ideal for severe environments.

Key Features:

  • Composition: Predominantly nickel with chromium, molybdenum, titanium, and aluminum. These elements contribute to the alloy’s high strength and resistance to heat and corrosion.
  • Temperature Resistance: Effective in applications up to 1100°C (2012°F), maintaining mechanical integrity and stability.
  • Mechanical Properties: Offers high tensile and yield strength, ensuring reliability under extreme stress conditions.
  • Oxidation and Corrosion Resistance: Excellent resistance to oxidation and good resistance to corrosion, extending the life of components.
  • Applications: Commonly used in aerospace engines, industrial gas turbines, and high-temperature exhaust systems.
  • Heat Treatment: Can be heat-treated to achieve optimal strength and performance characteristics, providing versatility in manufacturing.

GH600 Alloy's advanced properties make it suitable for demanding aerospace and industrial applications, ensuring long-term performance and reliability in challenging environments.

Here’s a detailed composition table for GH600 Alloy:

Element Composition (%)
Nickel (Ni) Balance
Chromium (Cr) 14.0 - 16.0
Molybdenum (Mo) 4.0 - 5.0
Titanium (Ti) 1.8 - 2.5
Aluminum (Al) 1.0 - 1.5
Iron (Fe) ≤ 4.0
Carbon (C) ≤ 0.08
Silicon (Si) ≤ 0.50
Manganese (Mn) ≤ 0.50
Boron (B) ≤ 0.01

These values provide a general guideline, but exact specifications can vary slightly based on the manufacturer's standards and requirements.

Round Nickel Alloy Rod GH600 Alloy Anti Oxidation Nickel Based Superalloy

Send your message to this supplier
Send Now

Round Nickel Alloy Rod GH600 Alloy Anti Oxidation Nickel Based Superalloy

Ask Latest Price
Brand Name :
Zhonggong Special Metallurgy
Model Number :
GH600 Alloy
Place of Origin :
China
MOQ :
100KG
Price :
Price is negotiated based on the required specifications and quantity
Payment Terms :
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Contact Supplier
Round Nickel Alloy Rod GH600 Alloy Anti Oxidation Nickel Based Superalloy
Round Nickel Alloy Rod GH600 Alloy Anti Oxidation Nickel Based Superalloy

Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.

Active Member
2 Years
jiangsu, wuxi
Since 2010
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Other, Seller, Trading Company
Total Annual :
1000000-1500000
Employee Number :
100~200
Certification Level :
Active Member
Contact Supplier
Submit Requirement