Specifications
Brand Name :
Zhonggong Special Metallurgy
Model Number :
GH36 Alloy
Place of Origin :
China
MOQ :
100KG
Price :
Price is negotiated based on the required specifications and quantity
Payment Terms :
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability :
5000 tons per month
Delivery Time :
5-8 working days, depending on the parameters required for negotiation
Packaging Details :
Standard export packaging, or packaging as required
Certification :
ISO Certificate
Density :
~8.9 g/cm³ (0.321 lb/in³)
Melting Point :
~1350-1450°C (2460-2640°F)
Tensile Strength :
~850 MPa (123 ksi)
Yield Strength :
~700 MPa (102 ksi)
Elongation :
~15%
Thermal Conductivity :
~14 W/m·K (8.4 BTU·in/hr·ft²·°F)
Modulus of Elasticity :
~210 GPa (30 x 10³ ksi)
Corrosion Resistance :
Good oxidation and corrosion resistance at high temperatures
Applications :
Aerospace, gas turbines, and high-temperature structural components
Description

GH36 Alloy is a high-performance nickel-based superalloy renowned for its exceptional mechanical properties and resistance to high-temperature environments. It is specifically designed to offer high strength and durability in demanding applications such as aerospace and industrial machinery.

Key Properties and Features:

  • High-Temperature Strength: GH36 Alloy maintains robust mechanical properties, including high tensile strength (~850 MPa or 123 ksi) and yield strength (~700 MPa or 102 ksi), at elevated temperatures up to approximately 1350-1450°C (2460-2640°F). This makes it suitable for components subjected to intense thermal stresses.

  • Oxidation and Corrosion Resistance: The alloy is highly resistant to oxidation and high-temperature corrosion, ensuring longevity and performance in harsh environments. This property is crucial for applications in gas turbines, jet engines, and other high-temperature systems where resistance to oxidative degradation is essential.

  • Mechanical Properties: GH36 exhibits good elongation (~15%), contributing to its ability to withstand mechanical stresses and deformation without failure. This feature is important for structural integrity and reliability in critical applications.

  • Thermal Conductivity: With a thermal conductivity of approximately 14 W/m·K (10 BTU·in/hr·ft²·°F), GH36 efficiently manages heat dissipation, which is beneficial for maintaining thermal stability in high-performance applications.

  • Applications: Commonly used in aerospace components, high-temperature gas turbines, and other industrial applications where high strength, oxidation resistance, and thermal stability are required. GH36's combination of properties makes it a preferred choice for environments demanding exceptional performance and reliability.

GH36 Alloy's high strength and resistance to extreme conditions make it a trusted material for advanced engineering applications, providing durability and reliability in critical components exposed to severe environments.

Here’s a composition table for GH36 Alloy:

Element Composition Range (%)
Nickel (Ni) 60.0 - 65.0
Chromium (Cr) 15.0 - 20.0
Cobalt (Co) 5.0 - 10.0
Molybdenum (Mo) 2.0 - 4.0
Iron (Fe) ≤ 6.0
Titanium (Ti) 1.0 - 2.0
Aluminum (Al) 1.0 - 2.0
Carbon (C) ≤ 0.10
Manganese (Mn) ≤ 0.5
Silicon (Si) ≤ 0.5
Sulfur (S) ≤ 0.01

These values provide general guidelines. For precise specifications or detailed applications, consult specific standards or suppliers.

Oxidation Resistance Nickel Alloy Pipe GH36 Alloy Nickel Based Superalloy

Send your message to this supplier
Send Now

Oxidation Resistance Nickel Alloy Pipe GH36 Alloy Nickel Based Superalloy

Ask Latest Price
Brand Name :
Zhonggong Special Metallurgy
Model Number :
GH36 Alloy
Place of Origin :
China
MOQ :
100KG
Price :
Price is negotiated based on the required specifications and quantity
Payment Terms :
Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Contact Supplier
Oxidation Resistance Nickel Alloy Pipe GH36 Alloy Nickel Based Superalloy
Oxidation Resistance Nickel Alloy Pipe GH36 Alloy Nickel Based Superalloy

Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.

Active Member
2 Years
jiangsu, wuxi
Since 2010
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Other, Seller, Trading Company
Total Annual :
1000000-1500000
Employee Number :
100~200
Certification Level :
Active Member
Contact Supplier
Submit Requirement