Inconel 718 Alloy
Inconel 718 is a precipitation hardened nickel-based alloy designed to display exceptionally high yield, tensile and creep-rupture properties at temperatures up to 1300°F (704°C). The age-hardening response of Inconel 718 permits annealing and welding without spontaneous hardening during heating and cooling. Nickel Alloy 718 has excellent weldability when compared to the nickel-base super alloys hardened by aluminum and titanium.
Advantages of Inconel 718 Strips
Applications of Inconel 718 Strips
Chemical Properties of Inconel 718
Nickel (plus Cobalt) .......................................................50.00-55.00
Chromium......................................................................17.00-21.00
Iron .....................................................................................Balance
Niobium (plus Tantalum)....................................................4.75-5.50
Molybdenum .....................................................................2.80-3.30
Titanium.............................................................................0.65-1.15
Aluminum ..........................................................................0.20-0.80
Cobalt ...............................................................................1.00 max.
Carbon..............................................................................0.08 max.
Manganese .......................................................................0.35 max.
Silicon ...............................................................................0.35 max.
Phosphorus.....................................................................0.015 max.
Sulfur...............................................................................0.015 max.
Boron ..............................................................................0.006 max.
Copper..............................................................................0.30 max
| Density | 8.19g/cm³ | 0.296 lb/in³ |
| Melting point | 1260-1336 | 2437°F |
Inconel series
Customize size as below
| Shape | Size(mm) |
| WIre | 0.5-7.5 |
| Rod/Bar | 8.0-200 |
| Strip | (0.5-2.5)*(5-180) |