Advantages of Inconel 718 Strips
High Strength-to-Weight Ratio: Provides durability without adding excessive weight.
Excellent Fabricability: Can be easily machined and formed into complex shapes.
Resistance to Oxidation and Corrosion: Ensures longevity in challenging environments.
Applications of Inconel 718 Strips
Aerospace Components
Thrust Reversers: Used in thrust reversers for jet engines, where high-temperature resistance and strength are essential.
Structural Components: Fabricated into various structural parts that require lightweight yet strong materials.
Oil and Gas Industry
Downhole Equipment: Employed in valves, fittings, and other components exposed to harsh environments.
Subsea Applications: Ideal for use in subsea pipelines and connectors due to its excellent corrosion resistance.
Nuclear Applications
Fuel Rods and Structural Supports: Used in nuclear reactors where materials must withstand extreme conditions.
Marine Applications
Components in Marine Engines: Suitable for various parts exposed to seawater, where corrosion resistance is vital.
High-Performance Engineering
Fasteners and Bolts: Can be used to manufacture bolts and fasteners that require superior mechanical properties.
Heat Exchangers
Heat Exchanger Tubes: Utilized in heat exchangers where high temperatures and corrosive fluids are present.
Chemical Properties of Inconel 718
Nickel (plus Cobalt) .......................................................50.00-55.00
Chromium......................................................................17.00-21.00
Iron .....................................................................................Balance
Niobium (plus Tantalum)....................................................4.75-5.50
Molybdenum .....................................................................2.80-3.30
Titanium.............................................................................0.65-1.15
Aluminum ..........................................................................0.20-0.80
Cobalt ...............................................................................1.00 max.
Carbon..............................................................................0.08 max.
Manganese .......................................................................0.35 max.
Silicon ...............................................................................0.35 max.
Phosphorus.....................................................................0.015 max.
Sulfur...............................................................................0.015 max.
Boron ..............................................................................0.006 max.
Copper..............................................................................0.30 max
| Density | 8.19g/cm³ | 0.296 lb/in³ |
| Melting point | 1260-1336 | 2437°F |
Inconel series
Customize size as below
| Shape | Size(mm) |
| WIre | 0.5-7.5 |
| Rod/Bar | 8.0-200 |
| Strip | (0.5-2.5)*(5-180) |
| Tube | custom made |
| Plate | custom made |