Differential Scanning Calorimeter for Polymer Thermal Testing
This advanced touch-screen DSC instrument is specifically engineered for measuring oxidation induction time in polymer materials. Featuring one-touch automated operation, the system executes complete test workflows through its integrated software module.
Standards Compliance
- GB/T 19466.2‑2009 / ISO 11357‑2:1999
- GB/T 19466.3‑2009 / ISO 11357‑3:1999
- GB/T 19466.6‑2009 / ISO 11357‑6:1999
Key Features
- Industrial-grade wide-format touch display with comprehensive real-time data visualization
- USB communication port with auto-reconnect for stable data transmission
- Compact furnace assembly with configurable heating and cooling rates
- Electric heating with compressor-refrigerated circulating water cooling
- Dual temperature probes for outstanding repeatability in sample temperature acquisition
- Built-in gas flow meter for rapid two-channel gas switching
- Software compatible with multiple operating systems and display resolutions
- Customizable instrument operation sequences for fully automated workflows
- Fully-enclosed support framework to prevent furnace contamination
Technical Parameters
| Temperature range |
0℃~500℃ |
| Temperature resolution |
0.01℃ |
| Heating rate |
0.1~40℃/min |
| Cooling rate |
0.1~20℃/min |
| Calorimetric resolution |
100% |
| Constant temperature |
5℃~500℃ |
| Temperature control mode |
Heating, cooling, constant temperature |
| DSC range |
0~±500mW |
| DSC resolution |
0.01mW |
| Working power |
AC 220V 50Hz 300W or other |
| Atmosphere control gas |
Two-channel automatic control (nitrogen and oxygen) |
| Gas flow |
0-200mL/min |
| Gas flow accuracy |
0.2mL/min |
| Crucible |
Aluminium crucible Φ6.6*3mm |
| Calibration standard |
Standard material (indium, tin, zinc) |
| Data interface |
Standard USB interface |
| Display mode |
7-inch touch screen |
Standard Configuration
| DSC machine |
1 set |
| Aluminium crucibles |
300 pieces |
| Power cords and USB cable |
Each one |
| CD (software and operations video) |
One |
| Oxygen airway and nitrogen airway |
Each 5m |
| Operation manual |
One |
| Standard samples (indium, tin, zinc) |
Each one |
| Tweezer and medicine spoon |
Each one |
| External circulation thermostat sink |
One |
Furnace Bracket