Specifications
Brand Name :
ABOOM
Model Number :
Nimonic90
Certification :
EN 10204 Type 3.1
Place of Origin :
CHINA
MOQ :
1000kgs
Price :
USD Negotiable
Payment Terms :
T/T
Supply Ability :
200 TONS PER MONTH
Delivery Time :
7-15dyas
Packaging Details :
Bare packing/bundle packing with woven bag/wooden or steel frame crate packing/plastic cap protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested.
TYPE OF MATERIAL :
nickel-chromium-cobalt base alloy
PRODUCT :
Nimonic90 / UNS N07090 / W. Nr.2.4632 alloy seamless pipe
STANDARD :
ASME SB 167
GRADE :
Nimonic90 / UNS N07090 / W. Nr.2.4632
Manufacturing process :
The steel melt shall be refined with AOD or equivalent.
Type Of Tube :
Straight Pipe, U Bend Pipe , Coil Pipe
Surface Finish :
Pickled And Annealed, Bright Annealed, Polished
Description

ASME SB 167 Nickel Chromium Cobalt Alloy UNS N07090 Nimonic90 / W. Nr.2.4632

Nimonic90 / UNS N07090 / W. Nr.2.4632 alloy seamless pipe customization

Nimonic 90*(UNS N07090/W. Nr.2.4632)

Introduction

NIMONIC 90 (UNS N07090/W. Nr. 2.4632) is a wrought nickel-chromium-cobalt base alloy strengthened by additions of titanium and aluminum. It has been developed as an age-hardenable creep resisting alloy for service at temperatures up to 920°C

Application

The alloy is used for turbine blades, discs, forgings, ring sections and hot-working tools. Also used to make Aerospace fasteners.

Equal grades

GH4090
Nickel Alloy 90
UNS N07090
Werkstoff Nr. 2.4632
Werkstoff Br. 2.4969
NiCr20Co18Ti

Chemical composition

C≤0.13 Cr=18.00~21.00 Co=15.00~21.00 Al=1.00~2.00
Ti=2.00~3.00 Fe≤1.50 Zr≤0.0150 B≤0.020
Si≤0.80 Mn≤0.40 Si≤0.015 P≤0.020
Cu≤0.200 Ni=Remainder

Standard

AMS 5829

Forms of product available

Plate, sheet, strip, bar, wire, rod, pipe, tube, forging.

Delivery

Available on request


UNS N07090  Nimonic 90  Cobalt Based  Superalloys For Turbine Blades

Send your message to this supplier
Send Now

UNS N07090 Nimonic 90 Cobalt Based Superalloys For Turbine Blades

Ask Latest Price
Brand Name :
ABOOM
Model Number :
Nimonic90
Certification :
EN 10204 Type 3.1
Place of Origin :
CHINA
MOQ :
1000kgs
Price :
USD Negotiable
Contact Supplier
UNS N07090  Nimonic 90  Cobalt Based  Superalloys For Turbine Blades
UNS N07090  Nimonic 90  Cobalt Based  Superalloys For Turbine Blades

Shanghai Aboom Metal prodcut co.,ltd

Active Member
7 Years
shanghai, shanghai
Business Type :
Manufacturer
Employee Number :
>100
Certification Level :
Active Member
Contact Supplier
Submit Requirement