Solid Fin Tube ASTM A335 P9 Fin Material CS Heat Recovery Steam Generator
Material Specifications
Base Pipe (ASTM A335 P9):
Chromium-molybdenum (Cr-Mo) alloy steel with good high-temperature strength and corrosion resistance.
Composition: ~9% Cr, ~1% Mo, balanced with Fe.
Common applications: Power plants, refineries, high-temperature/pressure services (up to ~650°C/1200°F).
Fin Tube Construction
Performance Considerations
Thermal Conductivity: CS fins have lower heat transfer efficiency than aluminum fins but are stronger.
Temperature Limits:
P9 Pipe: Up to 650°C (1200°F).
CS Fins: Max ~400°C (750°F); beyond this, oxidation/scaling occurs.
Corrosion Resistance:
P9 resists oxidation/sulfidation; CS fins may need coatings (e.g., galvanizing, aluminizing) in corrosive environments.
Applications:
- Heat Exchangers: Boilers, economizers, air heaters.
- Process Industries: Refineries, petrochemical plants (for high-temperature gas/liquid streams).
- Power Generation: Waste heat recovery systems.
Specifications:
All dimensions are in Inches and specification upon your requests. | |||
Tube OD | Fin Height | Fin Thickness | Fins per Pitch(Density) |
5/8 | 3/8,1/2 | .015/.016/ .020 | 4, 5, 6, 7, 8, 9, 10, 11, 12 |
3/4 | 3/8,1/2,5/8 | .015/.016/ .020 | 4, 5, 6, 7, 8, 9, 10, 11, 12 |
1 | 3/8,1/2,5/8 | .015/.016/ .020 | 4, 5, 6, 7, 8, 9, 10, 11 |
1 1/4 | 3/8,1/2,5/8 | .015/.016/ .020 | 4, 5, 6, 7, 8, 9, 10, |
1 1/2 | 3/8,1/2,5/8 | .015/.016/ .020 | 4, 5, 6, 7, 8, 9, 10, 11 |
1 3/4 | 3/8,1/2,5/8 | .015/.016/ .020 | 4, 5, 6, 7, 8, 9, 10 |
2 | 3/8,1/2,5/8 | .015/.016/ .020 | 4, 5, 6, 7, 8, 9, 10 |
Please email us for more information. |