| Chemical Composition (ASTM A240 F904L) | ||
| Element | Composition, % (min) | Composition, % (max) |
| Carbon (C) | - | 0.02 |
| Manganese (Mn) | - | 2 |
| Phosphorus (P) | - | 0.045 |
| Sulfur (S) | - | 0.035 |
| Silicon (Si) | - | 1 |
| Chromium (Cr) | 19 | 23 |
| Nickel (Ni) | 23 | 28 |
| Molybdenum (Mo) | 4 | 5 |
| Copper (Cu) | 1 | 2 |
| Nitrogen (N) | - | 0.1 |
| Iron (Fe) | Balance | |
| Mechanical Properties (ASTM A240 F904L) | ||
| Property | Requirement | Note |
| Tensile Strength, min | 71 ksi (490 MPa) | |
| Yield Strength (0.2% offset), min | 31 ksi (220 MPa) | |
| Elongation in 2 in. (50 mm), min | 35% | For plates ≤ 3/4 in. (19 mm) thick. Slightly lower for thicker plates. |
| Hardness, max | 90 HRB (Rockwell B) | Typical Brinell Hardness (HBW) is ~180. |
| Important Fabrication Note: To achieve these mechanical properties and optimal corrosion resistance, the material and any welded fabrications must be supplied in the solution-annealed condition. This involves heating to a suitable temperature (e.g., 1100-1150°C) and rapidly quenching. | ||
1. Water & Wastewater Treatment • Seawater Intake & Discharge Lines
2. Chemical & Petrochemical Processing
3. Offshore, Marine & Desalination • Desalination Plant high-pressure RO trains, inter-stage piping, and effluent lines.
4. Pulp & Paper Industry
5. Power Generation