Specifications
Brand Name :
SPEZILLA
Model Number :
Seamless Tube
Certification :
ISO9001:2008, PED 97/23/EC
Place of Origin :
CHINA
MOQ :
Negotiation
Price :
Negotiation
Payment Terms :
T/T or L/C
Supply Ability :
1000 TONS / MONTH
Delivery Time :
25 DAYS
Packaging Details :
PLY-WOODEN CASE / BUNDLE WITH PLASTIC CAP
Product Name :
Duplex Stainless Steel Tube
Materials :
2205
O.D. :
25.4mm
W.T. :
BWG16
Length MAX :
12000MM Max.
Surface :
Pickling,Annelaed
Pipe Finish :
Cold Drawn
Standard :
ASTM,AISI,DIN,EN
Type :
Seamless/Welded
Shape :
Round
Description

Cold Rolled duplex stainless steel 2205 Tubing Stress Corrosion For Heat Exchanger

Specifications of Duplex Stainless Steel Welded Tube

1. Standard: ASTM ASME
2. Grade: 630 / 631 / 2205 / 2507 / 17-4PH
ASTM A789, ASTM A790, ASTM A450, ASTM A530,
GB/T 14976, GB/T 14975, GB/T 13296, etc
3. OD: 8mm-1000mm
4. Wall thickness: 0.3mm-30mm
5. Length: max.18000mm or as demand

6. Surface finish: Polishing (180#,220#,240#,320#400#,600#), Hairline, acid pickled, etc.

2205 is the most widely used duplex (ferritic/austenitic) stainless steel grade. It finds applications due to both excellent corrosion resistance and high strength. The standard duplex S31803 composition has over the years been refined by many steel suppliers, and the resulting restricted composition range was endorsed as UNS S32205.Duplex S32205 gives better guaranteed corrosion resistance, but for much of the Duplex S31803 currently produced also complies with Duplex S32205. 2205 is not generally suitable for use at temperatures above 300ºC as it suffers from precipitation of brittle micro constituents, nor below -50ºC because of its ductile-to-brittle-transition.

Duplex Stainless Steel Tubing has a chemical composition of approximately equal parts of austenite and ferrite which is why it has twice the design strength of normal austenitic and ferritic stainless steel tubing. Duplex stainless steel tubings have a wide range of corrosion resistance levels. They also have high resistance to stress corrosion cracking that they might have received from its ferritic side. Duplex stainless steels are still very much in their developing stages and there are constantly different brands being promoted, this should continue till an accomplished and proven grade emerges. Duplex stainless steel tubes are used by a number of companies across the globe because they are very cost effective.

Item Description
Basic Information Material Grade TP304 , TP304L , TP304H , TP316 , TP316L , TP316Ti , TP309S , TP310S , TP321 , TP321H , TP347 , TP347H , S31803 , S32750 , S32205 etc
Outer Diameter

1/4"-4"

Wall Thickness BWG20-BWG10
Length Can be Produced as per customer’s requirement
Standard ASTM A213 ; ASTM A269 ; ASTM A312 ; ASTM A789 ; ASTM A790 ect .
Process Method Cold Drawn or Cold Rolled

This specification covers Seamless austenitic stainless steel tubing intended for high temperature usage such as boiler, superheater, heat exchanger, or condenser tubes.

SeaWorthy Polywooden Cases/In Bundle

  • Application:

    Boilers, heat exchanger, heaters or condensers.

  • Package

Specifications:

Specifications (ASTM/ASME) Duplex Stainless Steel Pipe
Alloy UNS Designation Material
Specification
Tubing
Specification
Pipe
Specification
2205 S31803/S32205 A 240/SA-240 A 270 A 790/SA-790
A 789/SA-789 A928/SA928

Chemical Compositions:

Chemical Composition (%) Duplex Stainless Steel Pipe
Alloy 2205 2205
UNS Designation S31803 S32205
Carbon (C) max. 0.030 0.030
Manganese (Mn) max. 2.00 2.00
Phosphorus (P) max. 0.030 0.030
Sulfur (S) max. 0.020 0.020
Silicon (Si) max. 1.00 1.00
Chromium (Cr) 21.0 - 23.0 22.0 - 23.0
Nickel (Ni) 4.5 - 6.5 4.5 - 6.5
Molybdenum (Mo) 2.5 - 3.5 3.0 - 3.5
Nitrogen (N) 0.08 - 0.20 0.14 - 0.20
Iron (Fe) Balance Balance

Cold Rolled duplex stainless steel 2205 Tubing Stress Corrosion For Heat Exchanger

Send your message to this supplier
Send Now

Cold Rolled duplex stainless steel 2205 Tubing Stress Corrosion For Heat Exchanger

Ask Latest Price
Brand Name :
SPEZILLA
Model Number :
Seamless Tube
Certification :
ISO9001:2008, PED 97/23/EC
Place of Origin :
CHINA
MOQ :
Negotiation
Price :
Negotiation
Contact Supplier
Cold Rolled duplex stainless steel 2205 Tubing Stress Corrosion For Heat Exchanger
Cold Rolled duplex stainless steel 2205 Tubing Stress Corrosion For Heat Exchanger
Cold Rolled duplex stainless steel 2205 Tubing Stress Corrosion For Heat Exchanger
Cold Rolled duplex stainless steel 2205 Tubing Stress Corrosion For Heat Exchanger

Spezilla Tube Co., Ltd. (Shanghai)

Verified Supplier
8 Years
shanghai, shanghai
Since 2011
Business Type :
Manufacturer, Exporter
Total Annual :
>3000000.00
Certification Level :
Verified Supplier
Contact Supplier
Submit Requirement