Product Name :
INCOLOY alloy 801 Alloy Round Bar
Grades :
INCOLOY alloy 801
Processing methods :
Shot blasted,Ground,Peeled,Machined,etc
Surface :
Rrough Turned,Grinding,Centreless Ground,etc
Profile :
Round Bar,Flat Bar,Forging Parts,Sheets Plates,etc
Price Term :
Ex-work,FOB, DDU etc.
Description

INCOLOY alloy 801 Alloy Round Bar 801 Superalloy Round Bar 801 Round Bar 801 Bar

Description

Our company provides INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar.

All of INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

  • Material:Metal,INCOLOY alloy 801 Alloy Round Bar 801 Superalloy Round Bar 801 Round Bar 801 Bar
  • Shape:Superalloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Length: Fixed length or random length or based on the customer's special requirement.

Products Details

INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.05
Cr (%): ≤ 20.5
Ni (%): ≤ 32.0
Cu (%): ≤ 0.150

Ti (%): ≤ 1.10

Fe(%): ≤ 45.5

Tensile strength, σb/≥ MPa: 450
Yield strength, σ0.2/MPa: 170
Elongation, δ ≥(%): 30.0
Reduction of area, ф ≥ (%): -
Hardness via heat treatment /HBW: -

Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801

Applications:

INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar

Superalloy is widely used to produce the high temperature components for gas turbine in the field of aviation, naval vessels and industry, such as turbine blade, guide blade, turbine disc, high pressure compressor disc, combustor, and also production of energy conversion devices, such as aerospace craft, rocket motor, nuclear reactor, petrochemical equipments, coaly transforming and so on.

Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801

INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar

FAQ

Q: How do you control the quality?

A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 801 Alloy Round Bar 801 Superalloy Round Bar 801 Round Bar 801 Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801

Packing method

Wooden Pallet BOX,based on the customer's special requirement,etc

Send your message to this supplier
Send Now

Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801

Ask Latest Price
Brand Name :
PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number :
INCOLOY alloy 801
Certification :
SGS,TUV,BV,ISO,MTC
Place of Origin :
China
MOQ :
Negotiations
Price :
Negotiations
Contact Supplier
Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801
Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801

Mianyang Baoheng New Material Technology Co.,Ltd

Active Member
5 Years
mianyang
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Trading Company
Total Annual :
5000000-8000000
Employee Number :
10~30
Certification Level :
Active Member
Contact Supplier
Submit Requirement