Specifications
Brand Name :
PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number :
AMS 5686
Certification :
SGS, TUV, BV, ISO, MTC
Place of Origin :
China
MOQ :
800kg
Price :
Negotiations
Payment Terms :
T/T
Supply Ability :
50000KGS/Month
Delivery Time :
Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
Packaging Details :
Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name :
AMS 5686 Superalloy Sheet Steel
Characteristic :
Corrosion and Heat resisitant
Heat treatment condition :
+N, +AT, etc
Processing methods :
Peeld, Milled, etc
Available Shapes :
Tubing, Steel plate, etc
Surface :
Grinded, Bright, etc
Description

AMS 5686 Superalloy Sheet Steel

Product Information

AMS 5686 steel has good high-temperature strength and oxidation resistance, and can operate for a long time without failure at high temperatures. Its high-temperature strength is higher than many other steels and can be used in high-temperature environments exceeding 1000 ℃. At the same time, AMS 5686 steel also has good corrosion resistance and superior performance when used in some chemically corrosive environments.


Size Range

Round bar / Wire rod (Diameter):1.0 mm to 1100 mm
Square bar / Flat bar: 1.0 mm to 1000 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T5.0 - 1500 mm X W3 - 1000 mm X L100-1000 mm
Sheet steel via cold rolled: T1.0 - 10 mm X W1 - 1000 mm X L100 - 800 mm
Steel strip via cold rolled: T3.0 - 10 mm X W1.0 - 1500 mm X L (or in coil form)
Length: Fixed length or random length or based on the customer's special requirement.


Chemical Composition and standard

AMS 5686

Mechanical Properties

SAE AMS 5686G

C(%): ≤0.08
Si(%): ≤1.00
Mn(%): ≤2.00
P(%): 0.03
S(%)≤: 0.025

Cr(%): 17.0~19.0
Ni(%): 10.0~13.0
Mo(%): ≤0.50

Cu(%): ≤0.50

Tensile strength,Rm/MPa: ≤758
Yield strength,Rp/MPa: -

Elongation, A/%: -

Reduction of area, ψ/%: -

Hardness HRC: -

AMS 5686 Superalloy Sheet Steel

Applications

AMS5686 is mainly used for manufacturing high-temperature mechanical components such as aviation engine components, turbine blades, and turbine discs


If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com


AMS 5686 Superalloy Sheet SteelAMS 5686 Superalloy Sheet Steel


AMS 5686 Superalloy Sheet Steel

Send your message to this supplier
Send Now

AMS 5686 Superalloy Sheet Steel

Ask Latest Price
Watch Video
Brand Name :
PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number :
AMS 5686
Certification :
SGS, TUV, BV, ISO, MTC
Place of Origin :
China
MOQ :
800kg
Price :
Negotiations
Contact Supplier
video
AMS 5686 Superalloy Sheet Steel
AMS 5686 Superalloy Sheet Steel
AMS 5686 Superalloy Sheet Steel

Mianyang Baoheng New Material Technology Co.,Ltd

Active Member
5 Years
mianyang
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Trading Company
Total Annual :
5000000-8000000
Employee Number :
10~30
Certification Level :
Active Member
Contact Supplier
Submit Requirement