Specifications
Brand Name :
PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number :
NiFeCr12Mo, W-Nr 2.4975, AISI 682, Incoloy 901, AMS 5660, UNS N09901
Certification :
SGS, TUV, BV, ISO, MTC
Place of Origin :
China
MOQ :
500kg
Price :
Negotiations
Payment Terms :
T/T
Supply Ability :
50000KGS/Month
Delivery Time :
Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
Packaging Details :
Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Characteristic :
Heat and Corrosion-resistant
Heat treatment condition :
+AT, +P, etc
Processing methods :
Ground, Milled, etc
Available Shapes :
Steel strip via cold rolled, Forging piece
Surface :
Polished, Black,
Material Category :
Austenitic Nickel-Based Alloys
Description

AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy

Describe

Alloy 901 / 2.4975 is a nickel-chromium-molybdenum alloy containing titanium.

Size Range

Round bar / Wire rod (Diameter): 8.0 mm to 1000 mm

Square bar / Flat bar: 8.0 mm to 1000 mm

Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.

Heavy/middle plate via hot rolled: T5 - 200 mm X W10 - 1000 mm X L1000-12000 mm

Sheet steel via cold rolled: T5 - 10 mm X W5 - 1000 mm X L1000 - 1000 mm

Steel strip via cold rolled: T0.5 - 8.0 mm X W10 - 200 mm X L (or in coil form)

Length: Fixed length or random length or based on the customer's special requirement.

Chemical Composition and standard

Incoloy 901/N90901/AISI 682

NiFeCr12Mo/2.4975 AMS 5660
ASTM Udimet 901 DIN EN 10095-2018 SAE AMS 5660L-2015


C(%): ≤0.10
Si(%): ≤0.40
Mn(%): ≤0.50
P(%)≤: 0.040
S(%)≤: 0.030
Cr(%): 11.0~14.0
Ni(%): 41.0~43.5

Mo(%): 5.30~6.50

Ti(%): 2.20~2.75

B(%): 0.01~0.02

Al(%): ≤0.35

Cu(%): ≤0.50

Fe(%): Remainder


C(%): ≤0.10
Si(%): ≤0.60
Mn(%): ≤2.0
P(%)≤: 0.02
S(%)≤: 0.01
Cr(%): 11.0~14.0
Ni(%): 40.0~45.0

Mo(%): 5.0~7.0

Ti(%): 2.35~3.1

Co(%): ≤1.0

Al(%): ≤0.35

Fe(%): Remainder

C(%): ≤0.10
Si(%): ≤0.60
Mn(%): ≤1.0
P(%)≤: 0.030
S(%)≤: 0.030
Cr(%): 11.0~14.0
Ni(%): 40.0~45.0

Mo(%): 5.0~7.0

Ti(%): 2.35~3.10

B(%): 0.01~0.02

Co(%): ≤1.0

Al(%): ≤0.35

Cu(%): ≤0.50

Pd(%): ≤5 ppm

Bi(%): ≤0.3 ppm

Se(%): ≤3 ppm

Fe(%): Remainder


AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy

Mechanical Properties

Tensile strength, σb/Mpa: ≥175

Yield Point, σs/Mpa: ≥ 125

Elongation, δ/%: 15

Reduction of Area,ψ/%: ≥19

Applications

  • aviation industry
  • ship industry
  • Industrial Sector Gas Turbines

Contact us

If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com

AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 SuperalloyAISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy


AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy

Send your message to this supplier
Send Now

AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy

Ask Latest Price
Watch Video
Brand Name :
PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number :
NiFeCr12Mo, W-Nr 2.4975, AISI 682, Incoloy 901, AMS 5660, UNS N09901
Certification :
SGS, TUV, BV, ISO, MTC
Place of Origin :
China
MOQ :
500kg
Price :
Negotiations
Contact Supplier
video
AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy
AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy
AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy

Mianyang Baoheng New Material Technology Co.,Ltd

Active Member
5 Years
mianyang
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Trading Company
Total Annual :
5000000-8000000
Employee Number :
10~30
Certification Level :
Active Member
Contact Supplier
Submit Requirement