Specifications
Brand Name :
PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number :
Udimet 710, ATG W4
Certification :
SGS, TUV, BV, ISO, MTC
Place of Origin :
China
MOQ :
600kg
Price :
Negotiations
Payment Terms :
T/T
Supply Ability :
50000KGS/Month
Delivery Time :
Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
Packaging Details :
Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name :
Udimet 710, ATG W4 Superalloy
Characteristic :
Anti-oxidation, Creep resistance
Heat treatment condition :
+P, +NT, etc
Processing methods :
Machined, etc
Available Shapes :
Steel plate, Sheet, Coil, etc
Surface :
Rrough Turned, Centreless Ground, etc
Description

Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips



Product Information

Udimet 710 superalloy has good oxidation resistance and creep resistance, and can be strengthened by precipitation hardening, solution hardening and work hardening. They also function under high mechanical stress and high temperature and where high surface stability is required


Size Range

Round bar / Wire rod (Diameter): 1.0 mm to 500 mm
Square bar / Flat bar: 1.0 mm to 500 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T3 - 1000 mm X W8 - 1000 mm X L800-12000 mm
Sheet steel via cold rolled: T5.0 - 8 mm X W5 - 1000 mm X L100 - 1000 mm
Steel strip via cold rolled: T0.3 - 8 mm X W10 - 1000 mm X L (or in coil form)
Length: Fixed length or random length or based on the customer's special requirement.


Chemical Composition and standard


Udimet 710

ATG W4

ASTM A959(2004)

JIS G4303(2005)


C(%): ≤0.07
Si(%): -
Mn(%): -
P(%)≤: -
S(%)≤: -
Cr(%):
≤18.0
Ni(%): ≤55.0
Mo(%): ≤3.0

W(%): ≤1.50

Al(%): ≤2.50

Ti(%): ≤5.0

Fe(%): ≤0.50

Co(%): ≤14.8

B(%): ≤0.02

C(%): ≤0.07
Si(%): -
Mn(%): -
P(%)≤: -
S(%)≤: -
Cr(%):
≤18.0
Ni(%): Remainder
Mo(%): ≤3.0

W(%): ≤1.50

Al(%): ≤2.50

Ti(%): ≤5.0

Fe(%): -

Co(%): -

B(%): ≤0.02


Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips
X120Mn12/1.3401 Mechanical Properties

Tensile strength, Rm/MPa: -
Yield strength, Rp/MPa: -
Elongation/%: -
Reduction of area, ψ/%: --

Impact, KV /J: -
Hardness, HBW: --


Applications

Udimet 710 is suitable for various high-temperature environments, such as steam and gas turbines.

If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com


Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled StripsUdimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips


Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips

Send your message to this supplier
Send Now

Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips

Ask Latest Price
Watch Video
Brand Name :
PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number :
Udimet 710, ATG W4
Certification :
SGS, TUV, BV, ISO, MTC
Place of Origin :
China
MOQ :
600kg
Price :
Negotiations
Contact Supplier
video
Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips
Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips
Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips

Mianyang Baoheng New Material Technology Co.,Ltd

Active Member
5 Years
mianyang
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Trading Company
Total Annual :
5000000-8000000
Employee Number :
10~30
Certification Level :
Active Member
Contact Supplier
Submit Requirement