It has a highly uniform structure and ultra-high porosity, it can be produced by a wide range of fiber weights and diameters and it has consistent fiber diameters.
| Diameter(u) | (g/m2) | |||
| 2 | 150 | 300 | 450 | 600 |
| 4 | 150 | 300 | 450 | 600 |
| 6 | 150 | 300 | 450 | 600 |
| 8 | 150 | 300 | 450 | 600 |
| 12 | 150 | 300 | 450 | 600 |
| 22 | 150 | 300 | 450 | 600 |
Widely used in gas-liquid separation, gas-solid separation and other industries.