Specifications
Brand Name :
Longsun
Model Number :
AgW Electrical Silver Contact Tips
Certification :
SGS, ISO9001,ROHS
Place of Origin :
CHINA
MOQ :
600PCS
Price :
Negotiable
Payment Terms :
L/C, T/T
Supply Ability :
2,000,000 pieces/month
Delivery Time :
Within 15 Working Days
Packaging Details :
Carton
Material :
Silver, Tungster
Types :
AgW, CuW, AgWC, AgWCC ect.
Usage :
Switchgears, Electronic Appliance.
Sample :
Available
Package :
Carton / As Required
Delivery :
TNT, DHL or Other Express
Description

Silver Alloy Contacts/Electrical Welding Button Contact/Silver Contact Sheets Used in Starters

Powder Metallurgy has already won more and more recognition in manufacturing method of contact material and became a main method for making Power Contact such as AgW, CuW, AgWC, AgWCC, AgNi, AgNiC, AgCetc.

Its characteristics as follows:

1. The component and quality of contact production made by Powder Metallurgy are more easy to control comparing with other manufacturing methods, because it can ensure uniformity of contact function. It is beneficial for ameliorating metallographic organization and improving function of contact materials by using advanced methods: chymic cladding, chemical sedimentation, pulverization, mechanization alloy.

2. Adopting the manufacturing methods of sinter and extrusion, their consistency can achieve 99.9%. Meanwhile, the second structure in silver base becomes fibre shape whose direction is vertical to the surface of Electrical Contacts, all these improve highly physical mechanism, arc corrosion resistance and low and stable resistance of the materials.

3. AgW, CuW, AgWC contacts choose different powder materials with adding inside Ni, Co mineral and by using pre-sinter and active sinter technology then improve their consistency and ameliorate electrical function of contact materials.

Application

1. AgW series: All kinds of omnipotence breakers, plastic breakers, heavy charge AC/DC contactorother switches.

2. CuW series: Widely used in high voltage breaker.

3. AgWCAgWCC series: Mainly used in high electricity charge switchgear such as breaker, creepage switch. Generally they are used with AgNi ,AgWC together.

4. AgNi series: Widely used in DC/AC relay, designation switch, contactor, light switch, thermal controller, timer of washer etc.

5. AgNiC series

Widely used in omnipotence breakers such as DW45 intelligence coupling with AgW.

6. AgC series

Mainly used in protective switch such as miniature breaker, creepage protective switch or motor protective switch with coupling contact in AgW.

Silver Electrical Contacts Powder Metallurgy Materials Welding With Contacts

Silver Electrical Contacts Powder Metallurgy Materials Welding With Contacts

Send your message to this supplier
Send Now

Silver Electrical Contacts Powder Metallurgy Materials Welding With Contacts

Ask Latest Price
Brand Name :
Longsun
Model Number :
AgW Electrical Silver Contact Tips
Certification :
SGS, ISO9001,ROHS
Place of Origin :
CHINA
MOQ :
600PCS
Price :
Negotiable
Contact Supplier
Silver Electrical Contacts Powder Metallurgy Materials Welding With Contacts
Silver Electrical Contacts Powder Metallurgy Materials Welding With Contacts
Silver Electrical Contacts Powder Metallurgy Materials Welding With Contacts
Silver Electrical Contacts Powder Metallurgy Materials Welding With Contacts

Wenzhou Longsun Electrical Alloy Co.,Ltd

Active Member
11 Years
zhejiang
Since 1986
Business Type :
Manufacturer, Exporter, Seller
Total Annual :
50 Million-70 Million
Employee Number :
300~500
Certification Level :
Active Member
Contact Supplier
Submit Requirement