Specifications
Brand Name :
Hanast
Model Number :
HN-8806AB
Certification :
ROHS SGS
Place of Origin :
GuangDong,China
MOQ :
1kg
Price :
Negotiable
Payment Terms :
T/T
Packaging Details :
25KG/barrel
Feature :
insulation, waterproof, corrosion resistance
Application :
Electronic components, solar energy
Appearance :
Grey fluid,black fluid,white fluid
Operating time :
30-40mins
Color :
can be customized
Sample :
free sample
Description

Factory Color Customized Flexible Electronic Potting Adhesive Two-Component Potting Compound Insulation Waterproof Corrosion Resistance Silicone Glue

PRODUCT DESCRIPTION

HN-8806, two-components addition type silicone potting rubber which can be cured into high-performance elastomer by room temperature or heating.

Customized Industrial Electronic Silicone Potting Compound Adhesive Corrosion Resistance

PRODUCT FEATURE

Excellent electrical insulation;

High moisture resistance: -50°C to 250°C;

Low viscosity ; Low shrinkage rate after curing;

No pollution in the surrounding environment.

Good thermal conductivity

Test Items Test Standard Units Product test results
Part A Part B

Before

Curing

1 Appearance By eyes --- Grey, fluid White, fluid
2 Viscosity GB/T10247- 2008 25ºC,mPa·S 4500~5000 4500~5000
3 Density GB/T 13354-92 25ºC,g/cm3 1.50±0.05 1.50±0.05
4 Mixing Ratio (A : B) 1:1 Weight ratio 100 100
Volume ratio 100 100
5 Operating time Measured hr 0.3-0.4
6 Curing condition Measured hr

4~12

(25ºC, initial cure)

0.20

(80ºC)

After

Curing

7 Appearance By eyes --- Grey Elastomer
8 Hardness GB/T 531.1-2008 Shore A 50±5
9 Thermal conductivity GB/T10297-1998 w/m·k ≥0.76
10 Expansivity GB/T20673-2006 µm/(m,ºC) 210
11 Moisture Absorption GB/T 8810-2005 24h,25ºC,% 0.01~0.02
12 Volume resistivity GB/T 1692-92 (DC500V),Ω· cm 1.0×1016
13 Dielectric intensity GB/T 1693-2007 Kv/mm(25ºC) 18~25
14 Temperature Resistance Measured ºC -50~+250

HOW TO USE​​

1. When used, weigh A and B according to proportion and then mix them evenly.

Mix thoroughly and evenly with a clean stirring device in a clean container, and then potting can be done.

It can also be sealed under a vacuum after removing the bubbles.

2. The surface of the potting element needs to be cleaned.

If the potting product is too large, it is recommended to potting in stages and then cure at room temperature (4-12hr) or by heating (80ºC-0.5hr).

3. For the automatic potting production line, in order to ensure accurate mixing ratio of A and B, Part A and Part B should be vacuumed respectively to remove the bubbles (the foaming time is 5-10 minutes), and then A and B should be pumped to the static mixer in proportion with a metering pump, and then potting can be done after mixing evenly.

Send your message to this supplier
Send Now

Customized Industrial Electronic Silicone Potting Compound Adhesive Corrosion Resistance

Ask Latest Price
Watch Video
Brand Name :
Hanast
Model Number :
HN-8806AB
Certification :
ROHS SGS
Place of Origin :
GuangDong,China
MOQ :
1kg
Price :
Negotiable
Contact Supplier
video
Customized Industrial Electronic Silicone Potting Compound Adhesive Corrosion Resistance

Shenzhen Haneste New Material co.,LTD

Verified Supplier
1 Years
guangdong, shenzhen
Since 2010
Business Type :
Manufacturer
Total Annual :
5000000-10000000
Employee Number :
50~100
Certification Level :
Verified Supplier
Contact Supplier
Submit Requirement