Product parameters
| Items | Parameters |
| Cleaning Power | 50W |
| Current Consumption | Pout = Ponm / 5A |
| Max. Power | 400W |
| Power Voltage | AC 110/220V |
| Cooling Method | Air Cooling |
| Laser Class | Level 4 |
| Pulse Energy | 1.5mJ |
| Fiber Optical Cable | 5m(Customizable) |
| Laser Wavelength | 1064nm |
| Scan Width | 1-120mm |
| Preheat Time | 10-30s |
| Working Condition | A flat place without vibration and impact |
| Working Temperature | 0-60 ℃ |
| Storage Temperature | -10~+60℃ |
| Machine size | L462 x W 260 x H562 (855mm with pull rod) |
| Net Weight | 32Kgs |
| Base Material | Surface Condition | Effective focus depth(mm) | Standard cleaning efficiency (mm/min) | High-speed cleaning efficiency(mm/min) | Cleaning effect |
| Cast iron | Heavy rust (0.08mm thickness) | >35 | 2000 | 3000 | Clean surface, no damage to the base metal |
| Carbon steel | Moderate corrosion (0.05mm thickness) | >40 | 2000 | 2500 | Clean surface, no damage to the base metal |
| Stainless steel | Surface oil, slightly rust | >50 | 2000 | 2800 | Clean surface, no damage to the base metal |
| Mold steel gear | Moderate oil stain, attached iron filings | >40 | 3000 | 3200 | Clean surface, no damage to the base metal |
| Aluminum plate | Oxide/surface contamination | >35 | 2500 | 3000 | Clean surface, no damage to the base metal |
| No putty paint layer | White pigmented paint (0.1mm thickness) | >20 | 1800 | 2000 | Clean surface, no damage to the base metal |