Tm Concentration Tolerance (atm%) |
Tm:0.5~5at% |
|
Orientation |
[111]<5 |
|
Parallelism |
≤10 |
|
Perpendicularity |
≤5′ |
|
Surface Quality |
10-5 (MIL-O-13830A) |
|
Wavefront Distortion |
≤ 0.125/25 mm @632.8nm |
|
Surface Flatness |
/8@632nm |
|
Clear Aperture |
>95% |
|
Chamfer |
0.15±0.05mm |
|
Size |
D: 2~10mmL: 3~150mm |
|
Coatings |
AR0.25% @2m |
|
Crystal Structure |
Cubic |
|
Lattice Constants |
12.01 |
|
Density |
4.56±0.04g/cm3 |
|
Melting Point |
1970℃ |
|
Thermal Conductivity /W/m/K@20℃ |
14W/m/K@20℃; 10.5W/m/K@100℃ |
|
Specific Heat (J/g. cm3@0-20℃) |
0.59 |
|
Thermal Optical Coefficient(dn/dT) |
7.3×10-6/K |
|
Thermal Expansion |
[100]: 8.2×10-6/K@0~250℃ |
|
[110]: 7.7×10-6/K@0~250℃ |
|
|
[111]: 7.8×10-6/K@0~250℃ |
|
|
Hardness (Mohs) |
8.5 |
|
Young`s Modulus |
3.17×104Kg/mm2 |
|
Shear Modulus |
310GPa |
|
Extinction Ratio |
≥ 25dB @632.8nm |
|
Tensile Strength/Gpa |
0.13~0.26 |
|
Solubility |
Insoluble in water, slightly soluble in ordinary acids |
|
Poisson Ratio |
0.25 |
|
Thermal Shock Resistance |
790W/m |
|
Laser Transition |
3F43H6 |
|
Laser Wavelength |
1.87~2.16m |
|
Temperature Dependence of Refractive Index |
7.3 10-6/K |
|
Absorption Cross Section |
7.5×10-21cm2 |
|
Diode Pump Band |
785nm, 680nm |
|
Emission Cross Section@2013nm |
2.9×10-20 cm2 |
|
Fluorescence Lifetime |
11ms |
|
Refractive Index @632nm |
1.83 |