Specifications
Grade :
cobalt alloy 21
Use :
Ore Mining
Material Grade :
UMCo50,cobalt alloy1,3,6
Hardness :
HRC 40 - 60
Performance :
Better Wear Property and Higher Temperature
Cast Process :
Wax Lost Process
Surface Treatment :
Shot Blast
Corrosion Resistance :
High
Standard :
ASTM B392
Heattreatment :
Solution annealing and aging
Shape :
Irregular Shape/Spherical Powder
Service :
OEM\ODM
Appearance :
Silvery
Type :
Bolts
Brand Name :
Eternal Bliss
Model Number :
EB26036
Certification :
ISO9001-2008
Place of Origin :
China
MOQ :
30 kg
Price :
USD80/kg ~ USD120/kg
Payment Terms :
by T/T or L/C, Western Union
Supply Ability :
100,000,000.00
Delivery Time :
It depends on the quantity to be ordered.
Packaging Details :
Pallets
Wearresistance :
High
Usage :
Oil and Gas Industry
Quality Control :
100% Inspected
Thermalconductivity :
15 - 25 W/m·K
Drawing Made :
accept
Castingmethod :
Investment casting, sand casting
Description

Heat Treatment FSX-414 Cobalt Based Superalloy with Precision Castings EB26036

Heat Treatment FSX-414 Cobalt Based Superalloys Precision Metal Casting EB26036

The as-cast samples of FSX-414 Co-based superalloy were heat treated at the standard solution and aging heat treatment cycles. Specimens for joining were cut from the as-cast ingot. Transient liquid phase (TLP) bonding was carried out at the standard solution cycle, using MBF-30 interlayer. Also, bonded specimens were homogenized at the standard aging condition

We produce High Temperature Superalloy Castings Parts with centrifugal cast process, precision cast process and resin sand cast process.

Table 1 : Standard Cobalt cobalt alloy Alloy

Co Cr C W Mo Ni Si B Fe Mn Others
cobalt alloy 1 BAL 33 2.45 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 3 BAL 31 2.5 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 4 BAL 31.5 1 14 - 2.0* 1 - 2.0* 1 -
BAL 28 1.2 5 - 3.0* 1 - 2.5* 1 -
cobalt alloy 12 BAL 29 1.85 9 - 2.5* 1 - 2.5* 1 -
cobalt alloy 20 BAL 33 2.45 17.5 - 2.5* 1 - 2.5* 1 -
cobalt alloy 21 BAL 27 0.25 - 5.5 2.5* 1 - 3.0* 1 -
cobalt alloy 31 BAL 26 0.5 7.5 - 10.5 1 - 2.0* 1 -
cobalt alloy 190 BAL 26 3.3 14 - 1.0 1 - 8.0 0.5 -
cobalt alloy 238 BAL 26 0.1 - 3 - 1 - 20.0 1 -
cobalt alloy 306 BAL 25 0.4 2 - 6.0 1 - 4.0* 1 Nb=5
94 BAL 28 1 19 - 5.0 1 - 2.5* 1 V=1
cobalt alloy F BAL 25.5 1.75 12.25 - 22.5 1 - 1.5* - -
cobalt alloy SF1 BAL 19 1.3 13 - 13 3 2.5 3* 0.5 Cu=0.5
cobalt alloy SF6 BAL 19 0.7 7 - 13 2.5 1.7 3* 0.5 Cu=0.5
cobalt alloy SF12 BAL 19 1 9 - 13 3 2 3* 0.5 Cu=0.5
cobalt alloy SF20 BAL 19 1.5 15 - 13 3 3 2* 0.5 Cu=0.5
TRIBALOY T400 BAL 8 0.1* - 28 3* 2.4 - 3* - -
TRIBALOY T800 BAL 17 0.1* - 28 3* 3.2 - 3* - -
DELORO 15 - - 0.06* - - BAL 2.0 1.05 1.5* 20 Cu=20
DELORO 22 - 0.70 0.10 - - BAL 2.3 1.75 - - -
DELORO 40 - 7.0 0.10 - - BAL 3.5 2.25 - - -
DELORO 50 - 10.25 0.45 - - BAL 4.0 1.85 4.0 - -
DELORO 60 - 14.25 0.6 - - BAL 2.0 3.5 4.0 - -
DELORO 625 - 22 0.1 - 9 BAL - - 5 - -
NISTELLE C - 16.5 0.12* 4.5 17 BAL 0.7 - 6.0 - -
TRIBALOY T700 - 15 0.10* - 32 BAL 3.25 -
Hastelloy C22®(UNS N06022)(Max.)
C MN P S Si Cr Ni Mo CO Fe W V
0.015 0.5 0.02 0.02 0.08 20.0-22.5 Bal. 12.5-14.5 2.5 2.0-6.0 2.5-3.5 0.35
Hastelloy C276®(UNS N10276)(Max.)
C MN P S Si Cr Ni Mo CO Fe W V
0.01 1 0.04 0.03 0.08 14.5-16.5 Bal. 15.0-17.0 2.5 4.0-7.0 3.0-4.5 0.35
Hastelloyx®(UNS N06002)(Max.)
C MN P S Si Cr Ni Mo CO Fe W other
0.05-0.15 1 0.04 0.03 1 20.5-23.0 Bal. 8.0-10.0 0.5-2.5 17.0-20.0 0.2-1.0 /
Monel 400®(UNS NO4400) (Max.)
C MN S Si Ni Cu Fe
0.3 2 0.024 0.5 63 min 28-34 2.5
Monel M400®(UNS NO4400)(Max.)
C MN S Si Ni Cu Fe
0.3 2 0.024 0.5 63-70 28-34 2.5
Monel R405®(UNS NO4405)(Max.)
C MN S Si Ni Cu Fe
0.3 2 0.025-0.06 0.5 63.0min 28-34 2.5
Monel K500®(UNS NO5500)(Max.)
C MN S Si Ni Cu Ti AI Fe
0.1 2 0.01 0.5 63min 27-33 0.86 2.3-3.15 2
Inconel 600(UNS NO6600)(Max.)
C MN S Si Cr Ni Cu Fe
0.15 1 0.015 0.5 14-17 72 min 0.5 6.0-10.0
Inconel 601(UNS NO6601)(Max.)
C MN Si Cr Ni CO AI Fe
0.05 0.3 0.2 22.5 61.5min 5 1.4 14.1
Inconel 718(UNS NO7718)(Max.)
Cr Ni Mo CO Cb+Ta Ti AI Fe
19 52.5min 3.05 5 5.13 0.9 0.5 18.5
Chemical Analysis of Incoloy 800® uns(N08800)
C Cr Ni Ti AI Fe Grain
0.1 max 19.0-23.0 30.0-35.0 0.15-0.6 0.15-0.6 39.5min /
Incoloy800H® UNS(N08810)
C Cr Ni Ti AI Fe Grain
0.05-0.1 19.0-23.0 30.0-35.0 0.15-0.60 0.15-0.60 39.5min 5or coarser
Incoloy800HT® UNS(N08811)
C Cr Ni Ti AI Fe Grain
0.06-0.10 19.0-23.0 30.0-35.0 0.25-0.60 0.25-0.60 39.5min 5or coarser

Dimensions:as per drawings

Special Features:

1.Good surface finish;

2.We use Precision Cast Process to produce the Cobalt Based Superalloy parts.

3.We do high temperature solution treatment to achieve better wear performance.

Production Process

Step 1: Getting orders.

Step 2: Process design by technical department

Step 3: Purchase of raw materials and pattern making &checking

Step 4: Inspection of raw materials

Step 5: Melting by middle-frequency induction furnaces

Step 6: Ladle analysis by Spectrometer

Step 7: De-oxidization, slag-removal, tapping

Step 8: Pouring

Step 9: Openning & fettling

Step 10: Surface & dimensional check

Step 11: Heat treatment

Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)

Step 13: Packing

Step 14: Shipping

Heat Treatment FSX-414 Cobalt Based Superalloys Precision Metal Casting EB26036

1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.

Our Trade Show Heat Treatment FSX-414 Cobalt Based Superalloys Precision Metal Casting EB26036

Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.

Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

www.ebcastings.com


Eternal Bliss Alloy Casting & Forging Co.,LTD.

Add.: J-Sci-Tech Park, Binhu District,Wuxi,214122, Jiangsu,China
Send your message to this supplier
Send Now

Heat Treatment FSX-414 Cobalt Based Superalloys Precision Metal Casting EB26036

Ask Latest Price
Grade :
cobalt alloy 21
Use :
Ore Mining
Material Grade :
UMCo50,cobalt alloy1,3,6
Hardness :
HRC 40 - 60
Performance :
Better Wear Property and Higher Temperature
Cast Process :
Wax Lost Process
Contact Supplier
Heat Treatment FSX-414 Cobalt Based Superalloys Precision Metal Casting EB26036
Heat Treatment FSX-414 Cobalt Based Superalloys Precision Metal Casting EB26036
Heat Treatment FSX-414 Cobalt Based Superalloys Precision Metal Casting EB26036

Eternal Bliss Alloy Casting & Forging Co.,LTD.

Verified Supplier
9 Years
jiangsu, wuxi
Since 2013
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Trading Company, Seller
Total Annual :
3,000,000-6,000,000
Certification Level :
Verified Supplier
Contact Supplier
Submit Requirement