(After Secondary Sintering at 1500℃ + CVD Surface Treatment)
Sintering of ≥4.5-generation Lithium Iron Phosphate (LFP) cathode materials, graphite anode materials, and other materials requiring oxygen-free high-temperature calcination.
1000℃~3000℃
| Category | Item | Specification |
|---|---|---|
| Chemical Composition | Carbon Content | ≥99.9% |
| Physical Properties | Bulk Density | 1.75–1.79 g/cm³ |
| Flexural Strength | 30–50 MPa | |
| Compressive Strength | ≥80 MPa | |
| Oxidation Resistance | Excellent | |
| Thermal Conductivity | Superior | |
| Thermal Shock Resistance (above 1100℃) | Excellent |