Specifications
Surface Finish :
BA/ 2B/ NO.1/ NO.3/ NO.4/ 8K/ HL/ 2D/ 1D
Creep Strength :
≥200MPa
Corrosion Resistance :
Excellent
Alloy Type :
Nickel-based
Thickness :
According To Customer Needs
Fatigue Strength :
≥400MPa
Weldability :
Good
Width :
According To Customer Needs
Brand Name :
TISCO
Model Number :
201, 301L, 301, 310S, 316L, 316, 321, 436L, 304, 439, 436, 445
Place of Origin :
Shanxi, China
Certification :
CE
MOQ :
10 Tons
Price :
Negotiable
Packaging Details :
Standard waterproof package
Delivery Time :
3-7DAYS
Payment Terms :
L/C, T/T, Western Union
Supply Ability :
5000MT/Month
Description

Product Description:

Nickel-based superalloy is a kind of alloy that consists of nickel, chromium and other elements. It is widely used in various industries, such as petrochemical, aerospace and energy. Nickel-based superalloy has excellent strength and corrosion resistance, which makes it a perfect material for many applications. With its high creep strength of up to 200MPa, excellent elongation of up to 30%, and tensile strength of up to 1000MPa, Nickel-based superalloy can provide superior performance even under extreme conditions. It also features a wide range of surface finishes, from BA/2B/NO.1/NO.3/NO.4/8K/HL/2D/1D, so as to meet different customer needs. Moreover, its width can also be customized according to customer requirement. Nickel-based superalloy is a great choice for many applications, such as Nickel Chromium Based, Inconel 725 Nickel Based Superalloys Strip, and Corrosion Resistance Nickel Based Superalloys Plate and Round Bar.

Features:

  • Product Name: Nickel-based superalloy
  • Fatigue Strength: ≥400MPa
  • Creep Strength: ≥200MPa
  • Corrosion Resistance: Excellent
  • Weldability: Good
  • Elongation: ≥30%
  • SS304 316 Nickel Based Superalloys Industrial Square Tube
  • Nickel Based Superalloys Inconel 601 Strip
  • Nickel Based Superalloys Plate
  • Nickel Based Superalloys Bar

Technical Parameters:

Parameters Values
Width According To Customer Needs
Hardness ≤250HB
Surface Finish BA/ 2B/ NO.1/ NO.3/ NO.4/ 8K/ HL/ 2D/ 1D
Corrosion Resistance Excellent
Fatigue Strength ≥400MPa
Tensile Strength ≥1000MPa
Thickness According To Customer Needs
Alloy Type Nickel-based
Elongation ≥30%
Creep Strength ≥200MPa

Applications:

Nickel-based superalloy is an alloy composed of nickel and other elements, and is widely used in various industries such as aerospace, petrochemical, machinery, and power generation. The TISCO brand provides 201, 301L, 301, 310S, 316L, 316, 321, 436L, 304, 439, 436, 445 models of nickel-based superalloy strip with excellent weldability and superior corrosion resistance, and has passed CE certification. With a minimum order quantity of 10 tons, the price is negotiable and the delivery time is 3-7DAYS. The payment terms are L/C, T/T, Western Union and the supply ability is 5000MT/Month. The width of the strip can be customized according to customer needs, and the tensile strength and elongation can reach ≥1000MPa and ≥30%. The most popular nickel-based superalloys strip products include Inconel 601 Strip, Inconel 725 Nickel Based Superalloys Strip, and Inconel 625 Nickel Based Superalloys Strip.

Customization:

Nickel-based Superalloy

Are you looking for high-end Nickel-based superalloy? Look no further! TISCO offers the best Nickel-based superalloys made with premium quality materials. Our Nickel-based superalloy products include Inconel 725 Nickel Based Superalloys Strip, Round Bar Nickel Chromium Based Superalloy, and Nickel-based Superalloy Tube, which are all certified with CE.

The model numbers of the Nickel-based superalloy products range from 201, 301L, 301, 310S, 316L, 316, 321, 436L, 304, 439, 436, 445. The origin of the products is Shanxi, China. The minimum order quantity is 10 tons. The prices are negotiable. The standard packaging is a waterproof package. Delivery time is 3-7 days. Payment terms are L/C, T/T, and Western Union. Supply ability is 5000MT/Month. The tensile strength is ≥1000MPa. The alloys are Nickel-based. The width and thickness are customized according to customer needs. Corrosion resistance is excellent.

Support and Services:

Nickel-based superalloys are a type of alloy used in high-temperature applications. We provide technical support and services for this product, such as:

  • Expert consultation on product selection, processing and usage
  • Guidance on product design and application
  • Assistance in troubleshooting and solving technical issues
  • Provide comprehensive after-sales service

Packing and Shipping:

Packaging and Shipping

Nickel-based superalloys are typically packaged in sealed and labeled barrels or drums for transport. The packaging should be able to withstand the rigors of shipping, and should be clearly labeled with the product description and the supplier's contact information. The drums or barrels should also be clearly labeled with a hazardous material warning. The drums or barrels should be tightly sealed and should be placed on a pallet for easier transport.

FAQ:

Q: What is Nickel-based superalloy?

A: Nickel-based superalloy is a type of alloy that includes nickel and other elements, such as iron, chromium, and molybdenum. It is used in a variety of industrial applications, including aerospace, automotive, and nuclear power generation, due to its low expansion and excellent corrosion resistance.

Q: What is the brand name of the Nickel-based superalloy?

A: The brand name of the Nickel-based superalloy is TISCO.

Q: What are the model numbers of the Nickel-based superalloy?

A: The model numbers of the Nickel-based superalloy are 201, 301L, 301, 310S, 316L, 316, 321, 436L, 304, 439, 436, and 445.

Q: Where is the Nickel-based superalloy produced?

A: The Nickel-based superalloy is produced in Shanxi, China.

Q: What is the minimum order quantity of the Nickel-based superalloy?

A: The minimum order quantity of the Nickel-based superalloy is 10 Tons.

Send your message to this supplier
Send Now

Inconel 725 Nickel Based Superalloy Strip 2b Treatment 0.2mm With Excellent Corrosion Resistance

Ask Latest Price
Surface Finish :
BA/ 2B/ NO.1/ NO.3/ NO.4/ 8K/ HL/ 2D/ 1D
Creep Strength :
≥200MPa
Corrosion Resistance :
Excellent
Alloy Type :
Nickel-based
Thickness :
According To Customer Needs
Fatigue Strength :
≥400MPa
Contact Supplier
Inconel 725 Nickel Based Superalloy Strip 2b Treatment 0.2mm With Excellent Corrosion Resistance

Foshan Qunming Stainless Steel Co., Ltd

Site Member
5 Years
guangdong, foshan
Since 2010
Business Type :
Manufacturer, Exporter, Seller
Total Annual :
150000000-390000000
Employee Number :
110~120
Certification Level :
Site Member
Contact Supplier
Submit Requirement