HAMINOL 303G Fast Catalyzed Cure | 120–150°C Bake for Industrial Efficiency
HAMINOL 303G features a highly alkylated structure that enables rapid reaction with strong acid catalysts .
Recommended Application: 0.5-1.0% catalyst level on binder solids for a 15-20 minute bake at 120-150°C
- Low self-condensation tendency for improved performance
- Excellent film flexibility for superior coating durability
- Especially effective when combined with polyester resins for high-formability coatings