TZM alloy also widely used in aviation and other fields, such as nozzle material, nozzle material, valve body and gas pipe
Channel materials, grid materials in electronic tubes, X-ray rotating anode parts, die-casting and extrusion molds, heaters and heat shields in high-temperature furnaces, ion implantation etc.
Physical performance comparison between TZM alloy and Pure Molybdenum
| Material | Density (g/cm3) | Melting Point(℃) | boiling point(℃) | 
| TZM (Ti0.5/Zr0.1) | 10.22 | 2617 | 4612 | 
| Mo | 10.29 | 2610 | 5560 | 
| Mechanical property (TZM) | Elongation(%) | Elastic modulus(GPa) | Yield Strength (Mpa) | Tensile Strength(Mpa) | Fracture toughness(MP·m1/2) | 
| Value | <20 | 320 | 560~1150 | 685 | 5.8~29.6 | 
TZM (Ti0.5/Zr0.08) High temperature tensile strength and elongation
|  			 Temperature/℃  			 |  			 			 Properties  			 |  		|
|  			 Tensile Strength/MPa  			 |  			 			 Elongation/%  			 |  		|
|  			 RT  			 |  			 			 1140 ~1210  			 |  			 			 7.5~13.0  			 |  		
|  			 1000  			 |  			 			 700 ~720  			 |  			 			 5.2  			 |  		
|  			 1200  			 |  			 			320 ~360 |  			 			 9.0  			 |  		
|  			 1300  			 |  			 			 190 ~210  			 |  			 			 11.5 ~13.5  			 |  		
|  			 1400  			 |  			 			 140 ~170  			 |  			 			 11.0 ~16.0  			 |  		
TZM (Ti0.5/Zr0.1)Thermal and electrical properties
|  			 Properties  			 |  			 			 Coefficient of thermal expansion/K-1   			(20~100℃)  			 |  			 			 Thermal conductivity   			W/m·K  			 |  			 			 Maximum temperature in air   			℃  			 |  			 			 Resistivity   			Ω·m  			 |  		
|  			 Value  			 |  			 			 5.3X10-6  			 |  			 			 126  			 |  			 			 400  			 |  			 			 (5.3~5.5)X10-8  			 |  		
TZM Plate Parameters
| Thickness (mm) | Width (mm) | Length (mm) | 
| ≥0.02 | 150 | L | 
| 0.10-0.15 | 300 | 1000 | 
| 0.15-0.20 | 400 | 1000 | 
| 0.20-0.30 | 650 | 2540 | 
| 0.30-0.50 | 650 | 2540 | 
| 0.50-1.0 | 650 | 2540 | 
| 1.0 -2.0 | 600 | 2000 | 
| 2.0 -3.0 | 600 | 2000 | 
| > 3.0 | 600 | L | 
We also can make TZM customized parts according to drawings.