ASTM A182 – Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service
Grade: F51 Ferritic-Austenitic Stainless Steel
Chemical Requirements max, %
| Elements | F51 (S31803) | 
| Carbon | 0.030 | 
| Manganese | 2.00 | 
| Phosphorus | 0.030 | 
| Sulfur | 0.020 | 
| Silicon | 1.00 | 
| Nickel | 4.5-6.5 | 
| Chromium | 21.0-23.0 | 
| Molybdenum | 2.5-3.5 | 
| Nitrogen | 0.08-0.20 | 
Tensile and Hardness Requirements
| Grade Symbol | F51 (S31803) | 
| Tensile Strength,min, ksi [Mpa] | 90[620] | 
| Yield Strength, min,ksi [MPa] | 65[450] | 
| Elongation in 2 in.[50 mm] or 4D,min, % | 25 | 
| Reduction of Area, min, % | 45 | 