| Composition | Molybdenum doped silicates |
| Thermal stability | Luminous intensity retention ≥95% at 180℃ |
| Storage | Store In A Cool, Dry Place |
| Main peak wavelength (λp) | 507±2nm |
| Luminous efficiency | ≥135lm/W |
| Color purity (x, y) | x = 0.1780 ± 0.003, y = 0.6385 ± 0.003 |
| Excitation wavelength range | 440-470nm (peak wavelength: 455nm) |
| Applicable chips | 445~460 nm |
| Luminous intensity retention | after 2000 hours (85℃/85% RH): ≥92% |
| Applications: | Used in conjunction with nitrides to create high CRI and high brightness lighting products, or as mono-powder for green light production. |