1.Properties& Application:
(1). Apply to removing excessive calcium from aluminum and aluminum alloys.
(2). Excellent removing calcium function, as a rule, 15~20kg ACC can remove 1kg Calcium.
(3). After treatment by ACC, the dross is easy to be skimmed off, and the dross contains little aluminum.
2.Operation Instructions:
(1). Manual Operations: Put ACC powder into the aluminum molten, stirring molten to homogeneous, after reaction finish, keep the molten Al static for 5~10minutes.
(2). Inert Gas-Carrying: Jet the ACC powder into the molten aluminum by the jet device.
(3). Temperature: ≥730.
(4). Dosage: According to calculating and experimental results.
3.Package and Storage:
Appearance: white powder.
10kg/polythene bag. 20kg/carton.