Specifications
Brand Name :
SHUOBODA
Model Number :
DSC-200
Certification :
ISO/CE
Place of Origin :
China
MOQ :
1 set
Price :
Was programmed for 24h
Payment Terms :
L/C,T/T
Supply Ability :
500 sets/month
Delivery Time :
5~8 working days
Packaging Details :
Plywood box
Temperature range :
Room temperature of ~600℃
Temperature resolution :
0.001℃
Temperature fluctuation :
±0.001℃
Temperature repeatability :
±0.01℃
Heating rate :
0.1~100℃/min
The constant temperature time :
Was programmed for 24h
Description

DSC-200 Differential scanning calorimeter (DSC)

Product introduction

DSC-200 is one of the most accurate DSC series products launched by the company. The sensor is made of imported material E-pair, which has high accuracy, high sensitivity and good repeatability. The signal acquisition circuit has shielding protection, strong anti-interference, and extremely high baseline stability and repeatability.

DSC-200 differential scanning calorimeter can be used to test glass transition temperature, phase transition temperature, melting point, enthalpy value, curing temperature, product stability, oxidation induction period, etc. It is competent in the research of pipes, polymers, chemicals, food, medical treatment and many other fields, and its products serve universities, enterprises, third-party measurement and quality inspection units, with a wide range of applications to meet the testing needs of various industries.

Main Features

  • Industrial level of the 7-inch touch screen, display rich information
  • New furnace body structure, better baseline, higher accuracy. Heating adopts indirect conduction mode, high uniformity and stability, reduce pulse radiation, better than the traditional heating mode.
  • USB communication interface, strong versatility, reliable communication is not interrupted, support self-recovery connection function.
  • Automatic switching of two atmosphere flow rates, fast switching speed, short stability time. At the same time, increase the protective gas input.
  • Software is simple and easy to operate.
  • Ultra-high sensitivity, precision, 0.001 mw, 0℃.001
  • Exquisite technical indicators, superior performance, high-cost performance, widely used

Technical parameters

MODEL

DSC-200

Temperature range

Room temperature of ~600℃

Temperature resolution

0.001℃

Temperature fluctuation

±0.001℃

Temperature repeatability

±0.01℃

Heating rate

0.1~100℃/min

The constant temperature time

Was programmed for 24h

Temperature control mode

Heating up, constant temperature, cooling (fully automatic program control)

DSC range

0~±600mW

DSC, resolution

0.01uW

DSC, sensitivity

0.001mW

Working power supply

AC220V / 50Hz or customized

The atmosphere controls the gas

Nitrogen, oxygen (programmed / automatic switching)

Gas-flow rate

0-300mL/min

Gas pressure

0.2MPa

Display mode

24bit color, 7-inch LCD touchscreen display

Data interface

Standard USB interface

Parameter standard

Equipped with a standard material (indium, tin), the user can correct the temperature by himself

Optional Cooling device

Air cooling device (optional semiconductor -40~550℃, liquid nitrogen refrigeration -150~550℃)

Thermocouple

with multiple sets of thermocouples, temperature of a group of measured samples,One group to measure furnace temperature,One group measures the internal ambient temperature

Test map: Glass transition temperature

AC220V 50Hz DSC Differential Scanning Calorimetry Instrument RT 600℃

Test map: melting point and heat enthalpy

AC220V 50Hz DSC Differential Scanning Calorimetry Instrument RT 600℃

Lift temperature scan

AC220V 50Hz DSC Differential Scanning Calorimetry Instrument RT 600℃

AC220V 50Hz DSC Differential Scanning Calorimetry Instrument RT 600℃

Send your message to this supplier
Send Now

AC220V 50Hz DSC Differential Scanning Calorimetry Instrument RT 600℃

Ask Latest Price
Brand Name :
SHUOBODA
Model Number :
DSC-200
Certification :
ISO/CE
Place of Origin :
China
MOQ :
1 set
Price :
Was programmed for 24h
Contact Supplier
AC220V 50Hz DSC Differential Scanning Calorimetry Instrument RT 600℃
AC220V 50Hz DSC Differential Scanning Calorimetry Instrument RT 600℃

Shuoboda Instruments (Hunan) Co., Ltd.

Verified Supplier
2 Years
hunan, jincheng
Since 2013
Business Type :
Manufacturer, Exporter
Total Annual :
1,000,000-10,000,000
Employee Number :
1~99
Certification Level :
Verified Supplier
Contact Supplier
Submit Requirement