Specifications
Brand Name :
KAIXIN
Model Number :
KX-Alloy605
Certification :
ISO9001:2015
Place of Origin :
China
MOQ :
200KG
Price :
To negotiate
Payment Terms :
T/T, L/C
Supply Ability :
50~80TONS per MONTH
Delivery Time :
45~60days
Packaging Details :
Wooden Box, size as per guests request
Shape :
Wire, Strip, Rod, Tube, Plate
Alloy Type :
Nickel-based Deformed Superalloy
Raw Materials :
NI9-11%,CR19-21%,W14-16%,MO Rem
Executive Standard :
ASTM
Delivery State :
Sosoloid
Application :
Manufacture engine guide blade, turbine outer ring, outer wall, swirler, sealing plate and etc parts
Features :
Excellent stability and high strength
Size :
Negotiable
Description

KX GH605 Light Rod Plate Structural Operating Temperature Range For High Temperature Alloy

Product Description and Application

GH605 is also known as L605,UNSR30605,GH5605

GH605 is a Co-Cr-Ni based solid solution enhanced deformation superalloy, its use temperature is below 1000℃. Cobalt-based superalloy GH605 is a cobalt base alloy strengthened by solution of 20%Cr and 15%W(percent mass). It has medium durability and creep strength below 815℃, excellent oxidation resistance below 1 090℃, and satisfactory process properties such as forming and welding. It is a key material for aero engine, rocket engine, naval ship and industrial gas turbine. Its development and production status is one of the symbols on the metal materials development level in a country. It is used for manufacturing the high temperature parts of aero engine guide blade, turbine outer ring, outer wall, swirler and sealing plate.

Process Performance and Requirements

  • Product Fusion Process

Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)

  • Product Chemical Composition

Composition Fe C Si Mn P S Cr Ni W More
Min - 0.05 - 1 - - 19 9 14 Co:Rem
Max 3 0.15 0.4 2 0.04 0.03 21 11 16

  • Product Physical Property

Density p=9.13g/cm3
Melting Temperature Range 1330℃-1410℃

  • Product Mechanical Property

Variety Tensile Property in the Room Temperature

Hardness

HV

815℃ Durability Grain Size/Grade Other properties
MPa MPa MPa MPa t/h %
Middle Plate,Sheet,Strip ≧890 370-550 ≧35 ≤290 165 ≧24 ≧10 ≧2.5(1) Bend

Cold Hard Strip

Grade A

≧1500 ≧1300 ≧5 410-480 --- ---- --- ≧9 Bend

Cold Hard Strip

Grade B

≧1700 ≧1500 ≧3 485-560 --- --- --- ≧10 Bend
Bar ≧860 ≧340 ≧35 ≤ 282 165 ≧ 23 ≧10 ≧2(0) ---
Ring ≧860 ≧310 ≧30 ≤ 248 165 ≧ 24 ≧10 ≧2(0) ---

  • Productive Process

GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy

  • Professional Customization

Cold-drawn Wire ¢0.3~¢18mm(Delivery in rolls or trays)
Hot-Rolling Wire ¢5.5~¢20mm(Delivery in rolls)
Strip thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips)
Smooth Forged Rod on a Lathe

¢60~350mm,L800-2500mm

Hot-rolled Burnishing ¢20~80mm,L1000-5000mm
Cold Drawn and Burnishing ¢2.5~18mm,L1000-8000mm
Seamless Tube ¢1~275mm,wall thickness 0.2~30,L1000-8000mm

GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy

GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based SuperalloyGH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based SuperalloyGH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based SuperalloyGH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy

Send your message to this supplier
Send Now

GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy

Ask Latest Price
Brand Name :
KAIXIN
Model Number :
KX-Alloy605
Certification :
ISO9001:2015
Place of Origin :
China
MOQ :
200KG
Price :
To negotiate
Contact Supplier
GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy
GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy
GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy
GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy
GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy
GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy
GH605 Light Rod Plate High Temperature Alloy ASTM Nickel Based Superalloy

Danyang Kaixin Alloy Material Co., Ltd.

Verified Supplier
4 Years
jiangsu
Since 2007
Business Type :
Manufacturer, Trading Company
Total Annual :
10000000-30000000
Employee Number :
150~200
Certification Level :
Verified Supplier
Contact Supplier