Material :
Silicon Carbide and Graphite
Density :
2.21-2.25 g/cm3
Shape :
Cylindrical
Temperature Resistance :
Up to 1600°C
Application :
Nickel superalloy and turbine alloy melting
Alloy Type :
Nickel-Based Superalloys
Temperature Max :
1600C
Chemical Inertness :
Excellent
Description

Nickel Superalloy High Temperature SiC Graphite Crucible

Built for the extreme demands of nickel-based superalloy melting at temperatures up to 1600C. Exceptional chemical inertness prevents alloy contamination during critical aerospace material processing.

Key Features

  • 1600C maximum operating temperature
  • Excellent chemical inertness to Ni alloys
  • Resistant to Inconel/Hastelloy corrosion
  • Ultra-high purity graphite matrix
  • Thermal shock resistant for rapid cycling

Applications

Nickel superalloy melting, turbine blade casting, aerospace component manufacturing, nuclear-grade material processing.

Send your message to this supplier
Send Now

Nickel Superalloy High Temperature SiC Graphite Crucible 1600C for Aerospace Turbine

Ask Latest Price
Brand Name :
Baidun
Place of Origin :
China
Model Number :
NI-SP900
MOQ :
1 pcs
Price :
Negotiate
Payment Terms :
T/T
Contact Supplier
Nickel Superalloy High Temperature SiC Graphite Crucible 1600C for Aerospace Turbine

Qingdao Baidun Special Ceramics Technology Co., Ltd.

Active Member
3 Years
qingdao
Since 2007
Business Type :
Manufacturer, Exporter, Seller
Total Annual :
25000000-26000000
Employee Number :
120~130
Certification Level :
Active Member
Contact Supplier
Submit Requirement