GH600 Alloy is a high-performance nickel-based superalloy specifically designed for applications requiring exceptional strength and durability at high temperatures. It provides outstanding mechanical properties, thermal stability, and oxidation resistance, making it ideal for severe environments.
GH600 Alloy's advanced properties make it suitable for demanding aerospace and industrial applications, ensuring long-term performance and reliability in challenging environments.
Here’s a detailed composition table for GH600 Alloy:
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 14.0 - 16.0 |
| Molybdenum (Mo) | 4.0 - 5.0 |
| Titanium (Ti) | 1.8 - 2.5 |
| Aluminum (Al) | 1.0 - 1.5 |
| Iron (Fe) | ≤ 4.0 |
| Carbon (C) | ≤ 0.08 |
| Silicon (Si) | ≤ 0.50 |
| Manganese (Mn) | ≤ 0.50 |
| Boron (B) | ≤ 0.01 |
These values provide a general guideline, but exact specifications can vary slightly based on the manufacturer's standards and requirements.