FRP strength member/Fiber Reinforced Plastic FRP Rod
FRP Rod strength member is to use epoxy resin as foundation combined with the strength of glass fiber through pultrusion technology to produce a new type of high performance non-metallic composite material which is used to make various optical fiber cables.
Technical Parameter
| FRP Rod Test Item | Unit (or Condition) | Technical Parameter |
| Appearance | Uniform color, smooth surface, no bur, no crack | |
| Tensile Strength | MPa | ≥1100 |
| Elastic Tensile Modulus | GPa | ≥50 |
| Bending Strength | MPa | ≥1100 |
| Flexural Modulus | GPa | ≥50 |
| Elongation at Break | % | ≤4% |
| Coefficient of Linear Expansion | 1/°C (-30°C ~ +80°C) | ≤8×10-6 |
| Diameter Tolerance | % | ±2% |
| Specific Gravity | g/cm3 | 2.05~2.15 |
| Minimum Bending Radius | mm (28°C ± 5°C) | 40D |
| High Temperature Bending Performance | (50D, 100°C, 120h) | No bur, no crack, no break, smooth surface, back to original straight |
| Low Temperature Bending Performance | (50D, -40°C, 120h) |
No bur, no crack, no break, smooth surface, back to original straight |