Thickness :
3-120mm
Martensite-Ferritic :
Ss 405 , 409, 409L, 410, 420, 420J1 , 420J2 , 420F , 430 ,431...
Surface Finish :
No. 1, No. 4, No. 8, HL, 2B, BA
Standard :
ASTM, JIS, DIN, AISI, KS, EN
OEM :
YES
Name :
Stainless Steel Rod Bar
Description

2507 Stainless steel bar

2507 is a ferritic-austenitic (duplex) stainless steel. It combines the most beneficial properties of many ferritic steels and austenitic steels. Due to the high content of chromium and molybdenum, the steel has extremely high chromium and molybdenum content. Good resistance to pitting corrosion, crevice corrosion and uniform corrosion. The dual-phase microstructure ensures that the steel has a high resistance to stress corrosion cracking, and the mechanical strength is also high.
Product Features
Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar
Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Specifications of Stainless Steel Bar

Commodity

Stainless Steel Round Bar/Flat Bar/Angle Bar/Square Bar/Channel

Standard

AISI, ASTM, DIN, GB, JIS, SUS

Material

301, 304, 304L, 309S, 321, 316, 316L, 317, 317L, 310S, 201,202,321, 329, 347, 347H 201, 202, 410, 420, 430, S20100, S20200, S30100, S30400, S30403, S30908, S31008, S31600, S31635, etc.

Certification

SGS, BV, etc

Surface

Bright, Polished, Turn smooth(Peeled),Brush, Mill, Pickled etc.

Delivery Time

7-15 days after confirming the order.

Trade Time

FOB, CIF, CFR

Payment

T/T or L/C

MOQ

1 Ton

Specification

Item

Size

Finish

Stainless steel round bar

19*3mm-140*12mm

Black&Pickled&Bright

Stainless steel flat bar

19*3mm-200*20mm

Black&Pickled&Bright

Stainless steel square bar

Hot rolled: S10-S40mm

Cold rolled: S5-S60mm

Hot rolled&Annealed&Pickled

Stainless steel angle bar

20*20*3/4mm-180*180*12/14/16/18mm

White acid& Hot rolled&Polished

Stainless steel channel

6#, 8#, 10#, 12#, 14#, 16#, 18#, 20#, 22#, 24#

White acid& Hot rolled&Polished&Sandblast

Chemical Properties of Frequently-used Austenitic Stainless Steel Material Grade

ASTM

UNS

EN

JIS

C%

Mn%

P%

S%

Si%

Cr%

Ni%

Mo%

201

S20100

1.4372

SUS201

≤0.15

5.5-7.5

≤0.06

≤0.03

≤1.00

16.00-18.00

3.5-5.5

-

202

S20200

1.4373

SUS202

≤0.15

7.5-10.0

≤0.06

≤0.03

≤1.00

17.00-19.00

4.0-6.0

-

301

S30100

1.4319

SUS301

≤0.15

≤2.00

≤0.045

≤0.03

≤1.00

16.00-18.00

6.0-8.0

-

304

S30400

1.4301

SUS304

≤0.08

≤2.00

≤0.045

≤0.03

≤0.75

18.00-20.00

8.0-10.5

-

304L

S30403

1.4306

SUS304L

≤0.03

≤2.00

≤0.045

≤0.03

≤0.75

18.00-20.00

8.0-12.0

-

309S

S30908

1.4883

SUS309S

≤0.08

≤2.00

≤0.045

≤0.03

≤0.75

22.00-24.00

12.0-15.0

-

310S

S31008

1.4845

SUS310S

≤0.08

≤2.00

≤0.045

≤0.03

≤1.50

24.00-26.00

19.0-22.0

-

316

S31600

1.4401

SUS316

≤0.08

≤2.00

≤0.045

≤0.03

≤0.75

16.00-18.00

10.0-14.0

-

316L

S31603

1.4404

SUS316L

≤0.03

≤2.00

≤0.045

≤0.03

≤0.75

16.00-18.00

10.0-14.0

2.0-3.0

317L

S31703

1.4438

SUS317L

≤0.03

≤2.00

≤0.045

≤0.03

≤0.75

18.00-20.00

11.0-15.0

2.0-3.0

321

S32100

1.4541

SUS321

≤0.08

≤2.00

≤0.045

≤0.03

≤0.75

17.00-19.00

9.0-12.0

3.0-4.0

347

S34700

1.4550

SUS347

≤0.08

≤2.00

≤0.045

≤0.03

≤0.75

17.00-19.00

9.0-13.0

-

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Packing: seaworthy wooden pallets,water proof paper,pvc film,interleaving paper, in 20' or 40' container or as per customers' requirements.

-- 20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High)

-- 40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High)

-- 40ft HC:12032mm(Lengh)x2352mm(Width)x2698mm(High)

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Q1:How about the shipping fees?

Shipping costs will depend upon many factors. Express will be the quickest but will be most expensive. Sea freight is ideal for large quantities, but slower. Please contact us for specific shipping quotes, which are dependent upon quantity, weight, mode and destination.

Q2:What are your prices?

Our prices are subject to change depending on supply and other market factors. We will send you an updated price list after you contact us for further information.

Q3:Do you have a minimum order quantity?

Yes, we do have minimum orders for specific international products, please contact us for more information.

Send your message to this supplier
Send Now

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Ask Latest Price
Place of Origin :
Made in China
Brand Name :
Vespolari Jiangsu
Certification :
ISO SGS ROHS
MOQ :
1Ton
Price :
Negotiable
Payment Terms :
TT L/C
Contact Supplier
Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

Jiangsu Vespolari Steel Import & Export Co., Ltd.

Verified Supplier
5 Years
Since 2021
Business Type :
Manufacturer, Exporter, Trading Company, Seller
Total Annual :
6000000-10000000
Employee Number :
100~200
Certification Level :
Verified Supplier
Contact Supplier
Submit Requirement