Using Luberun substrate, Caso coating, Ashland glue, the most stable construction, stand the test of time products

Type | TPU-V7 | TPU-V8 | TPU-V9 | TPU-V10 | TPU-V8 PRO | |||
Thickness | 7mil | 7.5mil | 8.5mil | 10mil | 7.5mil | |||
Urethane | Aliphatic TPU | Aliphatic TPU | Aliphatic TPU | Aliphatic TPU | Aliphatic TPU | |||
Adhesive | Acrylic Adhesive | Acrylic Adhesive | Acrylic Adhesive | Acrylic Adhesive | Acrylic Adhesive | |||
Peel Strength | >25n/cm | >25n/cm | >25n/cm | >25n/cm | >25n/cm | |||
Coating Tech | Nano Ceramic Topcoat | Nano Ceramic Topcoat | Nano Ceramic Topcoat | Nano Ceramic Topcoat | Professional hydrophobic nano coating | |||
Tensile Strength | >20mpa | >22mpa | >24mpa | >30mpa | >22mpa | |||
Elongation Strength | >18n | >20n | >25n | >30n | >20n | |||
Repair performance | The wire brush is brushed back and forth 100 times, and the roasting gun can be completely repaired | |||||||
Elongation at Break | 200% | 225% | 230% | 235% | 225% | |||
Max Temperature | 110℃ | 110℃ | 110℃ | 110℃ | 110℃ | |||