NISSEI Screw And Barrel Assembly
Screw & Barrel Assembly Technical Specifications
| Component |
Material |
Main Alloy Composition |
Heat Treatment Process |
Hardness |
Surface Treatment |
Key Features |
| Screw |
KTL-202B All-Hard Alloy |
Cr 8.2%, V 1.2%, Mo 2%, Co 1% |
- Quenching: 1020–1050°C- Tempering: 550–570°C (≥3 times)- Tail annealed at high temperature |
HRC 60 ± 2 |
Titanium coating (Ti) |
Excellent wear resistance, enhanced corrosion resistance, extended service life |
| Screw Tip Assemblies |
KTL-202B All-Hard Alloy |
Cr 8.2%, V 1.2%, Mo 2%, Co 1% |
- Quenching: 1020–1050°C- Tempering: 550–570°C (≥3 times)- Tail annealed at high temperature |
HRC 60 ± 2 |
Titanium coating (Ti) |
High resistance to abrasion and pressure, improved durability under high-load conditions |
| Barrel |
KTL-ST30 Double Alloy (Fe-Ni Base) |
Inner alloy: Fe, Ni, Cr, C, Co, B |
— |
Base: HRC 26–28Inner layer: HRC 59–61 |
— |
- Alloy thickness: 1–2 mm (each side)- Low thermal expansion- High resistance to high-temperature softening |
| Flange |
Alloy Steel + Chromium Plating |
— |
- Heat treatment + electroplating |
Base: HRC 30–32Cr layer: HRC 62–64 |
Chromium plating (0.05–0.08 mm) |
Improved wear resistance and corrosion protection |
| Nozzle |
SKD61 |
— |
- Quenching: 1020–1050°C- Tempering: 550–570°C (≥2 times) |
HRC 50 ± 2 |
— |
Excellent thermal fatigue resistance and toughness |