Specifications
Applications :
aircraft fittings, gears, shafts, fuse parts, missiles, regulating valves, keys, aircrafts, aerospace
Categories :
Aerospace, Aluminum, Defense, Round Bar.
Weight-to-Strength Ratio :
Excellent
yield strength :
73,000 psi
tensile strength :
83,000 psi
shear strength :
48,000 psi
Brand Name :
HUANYU
Model Number :
HYRB7075
Place of Origin :
CHINA
MOQ :
1 METRIC TON
Price :
Negotiable
Payment Terms :
T/T
Supply Ability :
280 METRIC TON PER MONTH
Delivery Time :
40 DAYS
Packaging Details :
PLYWOOD CASE
Description

7075 Aluminum Round Bar High Strength And Good Stress Corrosion Control

Aluminum Round Bar 7075

is primarily used in the aerospace industry as it is the strongest Aluminumgrade. 7075 has the strength of many steels, while retaining Aluminum’s lightweight qualities and corrosion resistance.

Application on 7075 Aluminum Round Bar

  • Highly stressed structural parts
  • Aircraft fittings
  • Gears and shafts
  • Fuse parts
  • Meter shafts and gears
  • Missile components
  • Regulating valve parts
  • Worm gears
  • Other aerospace and aircraft parts

When forging this 7075 metal, it is recommended that the temperature be set between 700 and 900 degrees F. This should then be followed by solution heat treatment. It’s not recommended for welding to be used as a joining technique, but if needed, resistance welding can be used. It’s not recommended for arc welding to be used because it can lower the metal’s corrosion resistance.

Aluminum 7075 Chemical Composition:

  • Al balance
  • Zn 5.1-6.1%
  • Mg 2.1-2.9%
  • Cu 1.2-2.0%
  • Mn 0.30%
  • Fe 0.50%
  • Si 0.40%
  • Ti 0.20%
  • Cr 0.18-0.28%

Aerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion Control

Aerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion ControlAerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion Control

Send your message to this supplier
Send Now

Aerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion Control

Ask Latest Price
Applications :
aircraft fittings, gears, shafts, fuse parts, missiles, regulating valves, keys, aircrafts, aerospace
Categories :
Aerospace, Aluminum, Defense, Round Bar.
Weight-to-Strength Ratio :
Excellent
yield strength :
73,000 psi
tensile strength :
83,000 psi
shear strength :
48,000 psi
Contact Supplier
Aerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion Control
Aerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion Control
Aerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion Control

Chongqing Huanyu Aluminum Material Co., Ltd.

Verified Supplier
8 Years
chongqing
Since 1996
Business Type :
Manufacturer, Exporter, Seller
Total Annual :
80,000,000-120,000,000
Employee Number :
199~299
Certification Level :
Verified Supplier
Contact Supplier
Submit Requirement