Specifications
Brand Name :
GH3600
Certification :
COO, CCPIT
Place of Origin :
China
MOQ :
50 kgs
Price :
negotiation
Payment Terms :
Ex works/ FOB/ CPT
Supply Ability :
30,000 kgs/ month
Delivery Time :
25-30 days
Packaging Details :
Wooden box
Condition :
Bright/ Oxidized Soft/ Hard
Surface :
Bright
Diameter :
3-50mm
Shape :
Strip, Foil, Sheet, Wire, Bar.
Name :
Inconel 600 UNS N06600 GH3600
Description

High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator

Quick Detail:

Name

Inconel 600

UNS N06600

GH3600

Application

thermowell work in Erosion atmosphere; Anti-chlorine, hydrogen chloride, oxidation and carbonization corrosion; Nuclear reactor

Condition

Bright/ Oxidized

Soft/ Hard

Feature

GH3600 for a variety of corrosive media have corrosion resistance.

Petrochemical production of catalytic regenerator over 700 ℃ applications alloy 600 is recommended for longer life.

Shape

Strip, Foil, Sheet, Wire, Bar.

Standard

Description:

Physical properties

>Density (g/cm3): 8.4

>Melting point (℃): 1370~1425

Chemical composition(%)

Grade

C

Si

Mn

P

S

Ni

Cr

Cu

Fe

GH3600

≤0.15

≤0.5

≤ 1

≤0.015

≤0.015

72

14~17

≤0.5

6~7

Mechanical properties

Yield Strength (Mpa)

Tensile Strength (Mpa)

Elongation, %

Hardness, HB

GH3600

Cold-rolling

240

550

30

≤195

As annealed

180

500

35

≤185

Specifications

Grade

GH3600

Size

Ф 3~50mm

MOQ

50 kgs

Condition

Soft/ Hard; Bright/ Oxidized

Superalloy- GH3600 Inconel 600 Bar for thermowell in corrosive environment

If you have any questions, pls let us know - sales@tankii.com

Looking forward to your inquiry!

Send your message to this supplier
Send Now

Superalloy- GH3600 Inconel 600 Bar for thermowell in corrosive environment

Ask Latest Price
Brand Name :
GH3600
Certification :
COO, CCPIT
Place of Origin :
China
MOQ :
50 kgs
Price :
negotiation
Payment Terms :
Ex works/ FOB/ CPT
Contact Supplier
Superalloy- GH3600 Inconel 600 Bar for thermowell in corrosive environment

Shanghai Tankii Alloy Material Co.,Ltd

Verified Supplier
12 Years
shanghai, shanghai
Since 1981
Business Type :
Manufacturer, Exporter
Total Annual :
8000000-100000000
Employee Number :
90~100
Certification Level :
Verified Supplier
Contact Supplier
Submit Requirement