P235GH SCHEDULE 40 STANDARD STEEL PIPE FITTINGS SCH80 1.0345 ELBOW TEE CS REDUCING TEE
P235GH SCHEDULE 40 STANDARD STEEL PIPE FITTINGS SCH80 1.0345 ELBOW TEE CS REDUCING TEE
Material Specifications
| Grade: |
P235GH |
| Number: |
1.0345 |
| Classification: |
Non-alloy quality steel |
| Density: |
7.85 g/cm³ |
Applicable Standards
- EN 10028-2: 2009 Flat products made of steels for pressure purposes. Non-alloy and alloy steels with specified elevated temperature properties
- EN 10216-2: 2014 Seamless steel tubes for pressure purposes. Technical delivery conditions. Non-alloy and alloy steel tubes with specified elevated temperature properties
- EN 10217-5: 2002 Welded steel tubes for pressure purposes. Submerged arc welded non-alloy and alloy steel tubes with specified elevated temperature properties
- EN 10217-2: 2002 Welded steel tubes for pressure purposes. Electric welded non-alloy and alloy steel tubes with specified elevated temperature properties
- EN 10253-2: 2007 Butt-welding pipe fittings. Non alloy and ferritic alloy steels with specific inspection requirements
- EN 10273: 2007 Hot rolled weldable steel bars for pressure purposes with specified elevated temperature properties
Chemical Composition (%) - EN 10028-2-2003
| Element |
Composition |
| C |
max 0.16 |
| Si |
max 0.35 |
| Mn |
0.6 - 1.2 |
| Ni |
max 0.3 |
| P |
max 0.025 |
| S |
max 0.015 |
| Cr |
max 0.3 |
| Mo |
max 0.08 |
| V |
max 0.02 |
| N |
max 0.012 |
| Nb |
max 0.02 |
| Ti |
max 0.03 |
| Al |
max 0.02 |
| Cu |
max 0.3 |
| Cr+Cu+Mo+Ni |
< 0.7 |
Mechanical Properties
Tensile Strength (Rm)
| Nominal Thickness (mm) |
Tensile Strength (MPa) (+N) |
| to 100 |
360-480 |
| 100 - 150 |
350-480 |
| 150 - 250 |
340-480 |
Minimum Yield Strength (ReH)
| Nominal Thickness (mm) |
Minimum Yield Strength (MPa) (+N) |
| to 16 |
235 |
| 16 - 40 |
225 |
| 40 - 60 |
215 |
| 60 - 100 |
200 |
| 100 - 150 |
185 |
| 150 - 250 |
170 |
Impact Energy (KV)
| Direction |
Temperature |
Impact Energy (J) |
| Transverse (+N) |
-20°C |
27 |
| 0°C |
27 |
| +20°C |
40 |
| Longitudinal |
-10°C |
28 |
| 0°C |
40 |
| +20°C |
47 |
Min. Elongation at Fracture (A): 24-25% (+N)
Equivalent Grades
| Region |
Standard |
Grade |
| EU EN |
P235GH |
|
| USA |
A285 / A285Gr.C |
|
| Germany DIN,WNr |
1.0345 / ASt35 HI / StE255 |
|
| Japan JIS |
SB410 / SGV410 / SPV235 / SPV24 |
|
| France AFNOR |
A37AP / A37CP |
|
| England BS |
141-360 / 161Gr.360 |
|
| Italy UNI |
Fe360-1KG / Fe360-1KW / FeE235 |
|
| Belgium NBN |
D37-1.2 / E37-1.2 |
|
| Spain UNE |
A37RCI |
|
| China GB |
20 |
|
| Sweden SS |
1330 / 1330-01 |
|
| Poland PN |
St36K |
|
| Czechia CSN |
11364 / 11366 |
|
| Finland SFS |
Fe37BP |
|
| Austria ONORM |
St35KW |
|
| Russia GOST |
12k |
|
| Inter ISO |
P3 |
|
| India IS |
Grade1 |
|